Study on Process to Improve Eutectic Carbide of Stainless Bearing Steel 9Cr18
更新时间:2026-01-21
    • Study on Process to Improve Eutectic Carbide of Stainless Bearing Steel 9Cr18

    • Special Steel   Vol. 43, Issue 6, Pages: 46-49(2022)
    • DOI:10.20057/j.1003-8620.2022-00150    

      CLC:
    • Received:16 September 2022,

      Online First:18 November 2022,

      Published:18 November 2022

    移动端阅览

  • 徐亮, 李涛, 马永强, et al. Study on Process to Improve Eutectic Carbide of Stainless Bearing Steel 9Cr18[J]. Special Steel, 2022, 43(6): 46-49. DOI: 10.20057/j.1003-8620.2022-00150.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Test and Study on Relative Hot Plasticity of MnS Inclusion in a New Free-Cutting Stainless Steel TBPS
Key Metallurgical Technologies for Smelting 1Cr13 Stainless Steel via ANS-OB Process
Effect of Cold-rolled Deformation on the Microstructure and Properties of GH4169 Alloy for Nuclear Power
The Influence of Deformation and Heating Temperature on the Impact Toughness of 2205 Duplex Stainless Steel
Effect of Melting Rate on Solidification Process of High Filled Ratio 06Cr18Ni11Ti Electroslag Remelting Ingot

Related Author

王辉绵
罗刚
Li Boyang
Fu Xianbin
Jin Zhe
Xu Mengchun
Teng Xingze
Lu Zhihao

Related Institution

太原钢铁(集团)有限公司先进不锈钢材料国家重点实验室
State Key Laboratory of Metallic Materials for Marine Equipment and Applications
Iron & Steel Research Institute of Ansteel Group
Beijing Baimtec Material Co., Ltd.
Institute of Functional Materials, Central Iron and Steel Research Institute Limited
0