Effect of Cold Drawing Deformation on Grain Size and Decarbonization Determination of 30CrMnSiNi2A Hexagonal Products
Forming and Phase Transition | 更新时间:2026-01-21
    • Effect of Cold Drawing Deformation on Grain Size and Decarbonization Determination of 30CrMnSiNi2A Hexagonal Products

    • Special Steel   Vol. 44, Issue 3, Pages: 109-113(2023)
    • DOI:10.20057/j.1003-8620.2022-00159    

      CLC:
    • Received:17 October 2022,

      Published:01 June 2023

    移动端阅览

  • Zhao Chengzhi,Zhang Yuchun,Li Jianxin,et al.Effect of Cold Drawing Deformation on Grain Size and Decarbonization Determination of 30CrMnSiNi2A Hexagonal Products[J].Special Steel,2023,44(03):109-113. DOI: 10.20057/j.1003-8620.2022-00159.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Process Practice for Microstructure Optimization of UNS N09925 Alloy Forgings in Oilfield Service Industry
The Effect of Solution Treatment Temperature on the Primary γ′ Phase and the Grain Structure in GH4251 Alloy
Exploration and Process Optimization of Mixed Crystal Reasons in Steel SCR420H for Cold Forging Three-pins Shaft
Ultra-fine Crystallization Forging Process of Maraging Steel 18Ni(250)
Effect of Heat Treatment Process on Microstructure and Properties of Forged 430F Ferritic Stainless Steel

Related Author

Zhang Jiawei
Yang Liang
Yu Jie
Wu Yinhu
Zhu Yuliang
Wang Shucai
Wang Hanxu
Li Xinyu

Related Institution

Central Iron & Steel Research Institute Co.,Ltd.
Fushun Special Steel Co.,Ltd.
Baowu Special Metallurgy Co., Ltd.
Jiangyin Xingcheng Special Steel Works Co., Ltd., Jiangyin
High Speed Aerodynamics Institute, China Aerodynamics Research and Development Center
0