Influence of Hot Deformation Process on Network Carbide of 100Cr6 Bearing Steel Wire
更新时间:2026-01-21
    • Influence of Hot Deformation Process on Network Carbide of 100Cr6 Bearing Steel Wire

    • Special Steel   Vol. 43, Issue 6, Pages: 60-65(2022)
    • DOI:10.20057/j.1003-8620.2022-00167    

      CLC:
    • Received:28 September 2022,

      Online First:21 November 2022,

      Published:21 November 2022

    移动端阅览

  • 左锦中, 何西, 赵阳, et al. Influence of Hot Deformation Process on Network Carbide of 100Cr6 Bearing Steel Wire[J]. Special Steel, 2022, 43(6): 60-65. DOI: 10.20057/j.1003-8620.2022-00167.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

3

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Determination and Application of High Temperature Thermoplasticity and Continuous Cooling Transition(CCT) Curve of 16MnCr5
Development of Hot-Rolled Wire Rods of 35CrMo Annealing-Free Cold Heading Steel for High-Strength Bolts
Features of Continuous Cooling Transformation (CCT) of High Carbon Steel 72A for Tyre Core Wire
Continuous Cooling Transformation Curves and Structure of Nb-V-Ti Microalloying 08MnCr High Strength Steel

Related Author

Wang Lijun
Guo Juncheng
Han Guangyang
Wang Ningtao
孔祥伟
林再勇
张剑锋
郑晓伟

Related Institution

Hebei Engineering Innovation Center for Wire Rod
Technical Centre, Xingtai Iron & Steel Co.,Ltd.
Wire Rod Plant of Xingtai Iron & Steel Co.,Ltd.
Sales department of Xingtai Iron & Steel Co., Ltd.
江阴兴澄特种钢铁有限公司线材研究所,江阴
0