Effect of High Temperature Homogenization on Microstructure and Properties of GH4710 Nickel Base Alloy
Forming and Phase Transition | 更新时间:2025-05-09
    • Effect of High Temperature Homogenization on Microstructure and Properties of GH4710 Nickel Base Alloy

    • Special Steel   Vol. 45, Issue 1, Pages: 87-93(2024)
    • DOI:10.20057/j.1003-8620.2022-00206    

      CLC: TG156
    • Received:08 November 2022,

      Published:30 January 2024

    移动端阅览

  • Gao Shoulei,Xu Xiaowei,Zhang Hong,et al.Effect of High Temperature Homogenization on Microstructure and Properties of GH4710 Nickel Base Alloy[J].Special Steel,2024,45(01):87-93. DOI: 10.20057/j.1003-8620.2022-00206.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

3

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of C and Mo Content on Microstructure and Short-term Properties of IN617 Heat-resistant Alloy

Related Author

Tang Zhengxin
Li Gen
Li Ling
He Guanze
He Xikou
Liu Qicong
Jia Lei

Related Institution

Institute for Special Steels, Central Iron and Steel Research Institute Co., Ltd. (CISRI)
Shanghai Nuclear Engineering Research & Design Institute Co
Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing
0