您当前的位置:
首页 >
文章列表页 >
Effect of Different Alloying Processes on Inclusions of 18Cr Ultra-pure Ferrite Stainless Steel during Refining Process
Smelting and Solidification | 更新时间:2026-01-21
    • Effect of Different Alloying Processes on Inclusions of 18Cr Ultra-pure Ferrite Stainless Steel during Refining Process

    • Special Steel   Vol. 44, Issue 3, Pages: 34-38(2023)
    • DOI:10.20057/j.1003-8620.2022-00207    

      CLC:
    • Received:05 December 2022,

      Published:01 June 2023

    移动端阅览

  • Zhang Jianlong,Chen Xingrun,Cheng Yunxia,et al.Effect of Different Alloying Processes on Inclusions of 18Cr Ultra-pure Ferrite Stainless Steel during Refining Process[J].Special Steel,2023,44(03):34-38. DOI: 10.20057/j.1003-8620.2022-00207.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect on Fatigue Failure Behavior Induced by Inclusions in GCr15 Bearing Steel Under Different Metallurgical Processes
High Temperature Mechanical Properties and Fracture Mechanism of 9Cr-2W-3Co Martensitic Heat-resistant Steel
Effect of LF Soft Bubbling Time on Inclusions in Tire Cord Steel LX82 A
Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel
The Metallurgical Mechanisms of Inclusions in the FGH4096 Alloy during Electron Beam Refining

Related Author

Wang Zheng
Chen feng
Shi Tao
Yin Qing
Hu Bin
Luo Haiwen
Geng Wei
Zhu Zhibao

Related Institution

Jiangying Xingcheng Special Steel Works Co., Ltd., Jiangying
Daye Special Steel Co., Ltd.
Changzhou Baoling Heavy & Industrial Machinery Co., Ltd.
School of Metallurgy and Ecological Engineering, University of Science and Technology Beijing
State Key Laboratory of Advanced Refractories, Wuhan University of Science andTechnology
0