Production Practice of 18CrNiMo7-6 Electroslag Process for High-speed Rail Gear Steel
Product Research and Development | 更新时间:2026-01-21
    • Production Practice of 18CrNiMo7-6 Electroslag Process for High-speed Rail Gear Steel

    • Special Steel   Vol. 44, Issue 3, Pages: 29-33(2023)
    • DOI:10.20057/j.1003-8620.2022-00208    

      CLC:
    • Received:22 December 2022,

      Published:01 June 2023

    移动端阅览

  • Wang Zhixiang,Nan hai,Zhang Jinwen.Production Practice of 18CrNiMo7-6 Electroslag Process for High-speed Rail Gear Steel[J].Special Steel,2023,44(03):29-33. DOI: 10.20057/j.1003-8620.2022-00208.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Current on the Cleanliness of Electroslag Ingots During Low Frequency Electroslag Remelting
Migration Law of Mg Element during Electroslag Remelting of Superalloys
Development of M42 and above 12.9 Grade High Hardenability 42CrMoVNb Bolt Steel
Effect of Refining Slag Basicity on the Molten Steel Cleanliness of GCr15SiMn Bearing Steel
Design of Slag System for FB2 Heat-resistant Steel Electroslag Remelting and Its Effect on Element Loss

Related Author

Wang Bingjie
Wang Yu
Xiang Miaomiao
Shi Xiaofang
Chang Lizhong
Gao Xiaoyong
Ren Weiwang
Zhang Lifeng

Related Institution

School of Metallurgical Engineering, Anhui University of Technology
School of Mechanical and Materials Engineering, North China University of Technology
School of Mechanical Engineering, Yanshan University, Qinhuangdao City
Institute for Special Steels,Central Iron and Steel Research Institute Co., Ltd.
Dongfang Electric Wind Power Co., Ltd.
0