您当前的位置:
首页 >
文章列表页 >
Controlled Rolling and Cooling Process Optimization of Non-annealed 12Cr1MoV Wire Rod Products for Boiler Flat Steel
Forming and Phase Transition | 更新时间:2025-05-09
    • Controlled Rolling and Cooling Process Optimization of Non-annealed 12Cr1MoV Wire Rod Products for Boiler Flat Steel

    • Special Steel   Vol. 45, Issue 1, Pages: 94-97(2024)
    • DOI:10.20057/j.1003-8620.2022-00235    

      CLC: TG356.4
    • Received:14 December 2022,

      Published:30 January 2024

    移动端阅览

  • Zhu Shuai,Li Yang,Wang Guangshun,et al.Controlled Rolling and Cooling Process Optimization of Non-annealed 12Cr1MoV Wire Rod Products for Boiler Flat Steel[J].Special Steel,2024,45(01):94-97. DOI: 10.20057/j.1003-8620.2022-00235.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

5

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Study on Continuous Cooling Phase Transition of 12Cr1MoV Pearlite Heat-resistant Steel
Effect of Austenizing Time on Structure and Properties of DP780 Cold Rolled Dual Phase Steel
High Temperature Properties of Slab of Stainless Steels and Application in Concasting Secondary Cooling Process

Related Author

Li Yaqiang
Li Yingying
Li Chuan
Han Baochen
Shi Jingqing
潘恩宝
邸洪双
蒋光炜

Related Institution

Department of Automotive Engineering , Hebei Vocational University of Technology and Engineering
Hebei Special Vehicle Modification Technology Innovation Center, Hebei Vocational University of Technology and Engineering
School of material science and engineering, Hebei University of Science and Technology, Shijiazhaung
Chengde Jianlong Special Steel Co., Ltd.
东北大学轧制技术及连轧自动化国家重点实验室
0