Development of ϕ800 mm Forging Bar for GCr15SiMn2 Bearing Steel Applied for High-power Wind Main Bearings
Product Research and Development | 更新时间:2026-01-21
    • Development of ϕ800 mm Forging Bar for GCr15SiMn2 Bearing Steel Applied for High-power Wind Main Bearings

    • Special Steel   Vol. 44, Issue 5, Pages: 39-42(2023)
    • DOI:10.20057/j.1003-8620.2023-00015    

      CLC: TF03+3;TG156.2
    • Received:14 February 2023,

      Published:01 October 2023

    移动端阅览

  • Tao Shijun,Xiao Aiping,Li Xu,et al.Development of ϕ800 mm Forging Bar for GCr15SiMn2 Bearing Steel Applied for High-power Wind Main Bearings[J].Special Steel,2023,44(05):39-42. DOI: 10.20057/j.1003-8620.2023-00015.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Mechanism of Si on the Cementite Type Transformation in As-cast High Carbon Chromium Bearing Steel
Research on Evaluation Method of Carbide Band in High Carbon Chromium Bearing Steel

Related Author

Xu Taixu
He Zhijun
Yang Xin
Qiao Xiya
Huang Yufei
张林
刘海
官跃辉

Related Institution

School of Materials and Metallurgy, University of Science and Technology Liaoning
Key Laboratory of Green Low-Carbon and Intelligent Metallurgy Liaoning Province,University of Science and Technology Liaoning
江阴兴澄合金材料有限公司线材研究所
江阴兴澄特种钢铁有限公司研究院办公室
0