Effect of Aging treatment on the Evolution of Precipitates in Super Duplex Stainless Steel
Forming and Phase Transition | 更新时间:2025-05-09
    • Effect of Aging treatment on the Evolution of Precipitates in Super Duplex Stainless Steel

    • Special Steel   Vol. 45, Issue 1, Pages: 77-81(2024)
    • DOI:10.20057/j.1003-8620.2023-00071    

      CLC: TG156.1
    • Received:28 April 2023,

      Published:30 January 2024

    移动端阅览

  • Luo Renzhi,Hu Wenhao,Wang Fuming,et al.Effect of Aging treatment on the Evolution of Precipitates in Super Duplex Stainless Steel[J].Special Steel,2024,45(01):77-81. DOI: 10.20057/j.1003-8620.2023-00071.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of N Content on Precipitation Behavior of Secondary Austenite in S32750 Duplex Stainless Steel
Production Practice of Duplex Stainless Steel Wire Rods ER2209 for Welding Application
Application of Duplex Stainless Steels in Manufacture of Equipment for Nuclear Power Station
Effect of Ti and/or Nb on Structure and Mechanical Properties of High Temperature Alloy 25Cr37Ni0.6Nb

Related Author

Song Zhigang
He Jianguo
Feng Han
Zheng Wenjie
Zhu Yuliang
Wu Xiaohan
严道聪
谢东西

Related Institution

Research Institute of Special Steels, Central Iron & Steel Research Institute Co., Ltd.
浙江青山钢铁有限公司
瑞浦科技特种钢研究院
环境保护部核与辐射安全中心
永兴特种不锈钢股份有限公司
0