Current Status and Prospects of Fatigue Performance for 300M Steel by Single Vacuum Process for Landing Gear of Commercial Aircraft
Product Research and Development | 更新时间:2026-01-21
    • Current Status and Prospects of Fatigue Performance for 300M Steel by Single Vacuum Process for Landing Gear of Commercial Aircraft

    • Special Steel   Vol. 44, Issue 5, Pages: 53-59(2023)
    • DOI:10.20057/j.1003-8620.2023-00123    

      CLC: TG142.1
    • Received:15 June 2023,

      Published:01 October 2023

    移动端阅览

  • Han Shun,Li Yong,Zhao Suwu,et al.Current Status and Prospects of Fatigue Performance for 300M Steel by Single Vacuum Process for Landing Gear of Commercial Aircraft[J].Special Steel,2023,44(05):53-59. DOI: 10.20057/j.1003-8620.2023-00123.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

3

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Influence of Sulfur Content on Inclusion and Fatigue Properties of 18CrNiMo7-6 Gear Steels
Production Process Practice of 42CrMoM Steel for 12.9 Grade High Strength Wind Power Fasteners
Comparative Analysis of 3%Cr Roller Steel by Rare Earth Refining and Electroslag Remelting
Effect of Mo Microalloying on High Temperature Mechanical Properties and Microstructure of 82B Steel
Effect of Austenizing Time on Structure and Properties of DP780 Cold Rolled Dual Phase Steel

Related Author

Xie Dirong
Shi Jie
Wang Maoqiu
Yu Wenchao
Peng Feng
Liu Yueyun
Guo Shibei
Liu Dan

Related Institution

Research Institute, Daye Special Steel Co., Ltd.
Hubei Provincial Key Laboratory of High-quality Special Steel
Institute of Metal Research, Chinese Academy of Sciences
Baosteel Roll Technology Co., Ltd.
School of Materials Science and Engineering, Guilin University of Technology
0