Effect of Aging Rolling Temperature on the Microstructure, Texture and Magnetic Properties of Low-temperature Grain-oriented Silicon Steel
Forming and Phase Transition | 更新时间:2025-05-09
    • Effect of Aging Rolling Temperature on the Microstructure, Texture and Magnetic Properties of Low-temperature Grain-oriented Silicon Steel

    • Special Steel   Vol. 45, Issue 3, Pages: 80-84(2024)
    • DOI:10.20057/j.1003-8620.2023-00181    

      CLC: TG142.1
    • Received:22 August 2023,

      Published:30 May 2024

    移动端阅览

  • Liu Huidan,Yin Licheng,Zhu Jiqiao,et al.Effect of Aging Rolling Temperature on the Microstructure, Texture and Magnetic Properties of Low-temperature Grain-oriented Silicon Steel[J].Special Steel,2024,45(03):80-84. DOI: 10.20057/j.1003-8620.2023-00181.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Product Thickness on Texture and Magnetic Properties of Non-Oriented Silicon Steel
Impact of the Annealing Temperature on the Magnetic and Mechanical Characteristics of Thin-gauge Non-oriented Electrical Steel
Effect of Forging Process on Microstructure and Properties of Fe10Cr10Co Soft Magnetic Alloy
Microstructure and Mechanical Properties of Heat Treatment Low-alloy Wear-resistant Steel NM450
Effect of Powder Treatment on Oxygen Content, Microstructure and Mechanical Properties of FGH95 Superalloy

Related Author

董爱锋
苗晓
申毅
张文康
Liu Xuming
Geng Zhiyu
Li Fuqiang
Sun Chao

Related Institution

太原钢铁(集团)冇限公司技术中心
Silicon Steel Division, Anshan Steel Co., Ltd.
Ansteel Beijing Research Institute Co., Ltd.
Xi'an Gangyan Special Alloy Co.,Ltd
State Key Laboratory of Refractory Materials and Metallurgy, Wuhan University of Science and Technology
0