您当前的位置:
首页 >
文章列表页 >
Mechanism of Si on the Cementite Type Transformation in As-cast High Carbon Chromium Bearing Steel
Smelting and Solidification | 更新时间:2025-05-09
    • Mechanism of Si on the Cementite Type Transformation in As-cast High Carbon Chromium Bearing Steel

    • Special Steel   Vol. 45, Issue 3, Pages: 15-21(2024)
    • DOI:10.20057/j.1003-8620.2023-00201    

      CLC: TG260
    • Received:20 September 2023,

      Published:30 May 2024

    移动端阅览

  • Xu Taixu,He Zhijun,Yang Xin,et al.Mechanism of Si on the Cementite Type Transformation in As-cast High Carbon Chromium Bearing Steel[J].Special Steel,2024,45(03):15-21. DOI: 10.20057/j.1003-8620.2023-00201.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Modification Effect and Mechanism of La-Ce on Inclusions in GCr15 Bearing Steel
Development of ϕ800 mm Forging Bar for GCr15SiMn2 Bearing Steel Applied for High-power Wind Main Bearings
Practice and Analysis of Light Calcium Treatment of 55Cr3 Aluminum Deoxidized Spring Steel
Feature of Structure of Eutectoid Pearlitic Steel After Equal Channel Angular Pressing at Ambient Temperature
Research on Evaluation Method of Carbide Band in High Carbon Chromium Bearing Steel

Related Author

Fu Jianxun
Tian Qianren
Wang Zifei
Dong Bingcheng
Wu Xiangyu
Tao Shijun
Xiao Aiping
Li Xu

Related Institution

Center for Advanced Solidification Technology,School of Materials Science and Engineering,Shanghai;University,& State Key Laboratory of Advanced Special Steel
Technical;Center of Shandong Steel Laiwu Branch
Technology center, Daye Special Steel Co., Ltd.
Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing
Research Institute, Nanjing Iron and Steel United Co., Ltd.
0