您当前的位置:
首页 >
文章列表页 >
Water Model Experiment of Bottom Blown Bubble Movement Behavior and its Effect on Mixing Uniformity
Smelting and Solidification | 更新时间:2025-05-09
    • Water Model Experiment of Bottom Blown Bubble Movement Behavior and its Effect on Mixing Uniformity

    • Special Steel   Vol. 45, Issue 3, Pages: 22-26(2024)
    • DOI:10.20057/j.1003-8620.2023-00256    

      CLC: TF715.1
    • Received:18 December 2023,

      Published:30 May 2024

    移动端阅览

  • Du Tinghui,Feng Lianghua,Wu Mingtao,et al.Water Model Experiment of Bottom Blown Bubble Movement Behavior and its Effect on Mixing Uniformity[J].Special Steel,2024,45(03):22-26. DOI: 10.20057/j.1003-8620.2023-00256.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0