Low-cost Non-vacuum Induction Furnace Smelting of High Molybdenum Content of Nickel-base Alloy
Smelting and Solidification | 更新时间:2025-05-09
    • Low-cost Non-vacuum Induction Furnace Smelting of High Molybdenum Content of Nickel-base Alloy

    • Special Steel   Vol. 45, Issue 5, Pages: 72-75(2024)
    • DOI:10.20057/j.1003-8620.2024-00006    

      CLC: TF741.7
    • Received:04 January 2024,

      Published:30 September 2024

    移动端阅览

  • Wang Shucai,Guo Jing,Wu Zhilong,et al.Low-cost Non-vacuum Induction Furnace Smelting of High Molybdenum Content of Nickel-base Alloy[J].Special Steel,2024,45(05):72-75. DOI: 10.20057/j.1003-8620.2024-00006.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Development of Voltage Swing Control System of 15 t Consarc ESR Furnace
Influence of ESR Slag on Cleanness of GCr15 Bearing Steel
A Study on Model of VOD Steelmaking Process for Stainless Steel
Development and Application of Premelted Slag for Electroslag Remelting Process
Optimization on Remelting Process of 1.1 t ESR Ingot of Blade Steel 1Cr12Ni2Mo2VN

Related Author

李宛州
王京春
林艳生
张洲
李德胜
汪质刚
董艳伍
肖爱平

Related Institution

清华大学自动化系
冶金自动化研究设计院
大冶特殊钢有限公司技术中心
东北大学冶金学院
北京科技大学冶金与生态工程学院
0