您当前的位置:
首页 >
文章列表页 >
Continuous Cooling Phase Transformation Behavior of 40Cr13 Plastic Mold Steel
Forming and Phase Transition | 更新时间:2025-05-09
    • Continuous Cooling Phase Transformation Behavior of 40Cr13 Plastic Mold Steel

    • Special Steel   Vol. 45, Issue 5, Pages: 113-118(2024)
    • DOI:10.20057/j.1003-8620.2024-00007    

      CLC: TG142
    • Received:04 January 2024,

      Published:30 September 2024

    移动端阅览

  • Su Mengmeng,Chen Wei,Tang Jiali,et al.Continuous Cooling Phase Transformation Behavior of 40Cr13 Plastic Mold Steel[J].Special Steel,2024,45(05):113-118. DOI: 10.20057/j.1003-8620.2024-00007.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Development of Pre-hardened and Ultra-thick 1.2311 Steel Plate Used for Plastic Mold Steel
Process Practice of the On-line Solid Solution of Superior Mirror Surface Plastic Mold Steel P80

Related Author

Han Fei
Liang Jian
Bao Siqian
Zhou Lian
Li Shengyan
Liu Xiaolin
Dong Fujun
Liao Sangsang

Related Institution

Faculty of Materials Science, Wuhan University of Science and Technology
Hunan Valin Xiangtan Iron and Steel Co.,Ltd.
Guangdong Xiongfeng Mold Steel Material Technology Co.,Ltd.
School of Architecture and Art Design,Hunan University of Science and Technology
Xinyu Iron & Steel Co.,Ltd
0