Research Progress on Numerical Simulation of Temperature Field during Directional Solidification of Nickel-based Single Crystal Turbine Blades
Overview | 更新时间:2025-05-09
    • Research Progress on Numerical Simulation of Temperature Field during Directional Solidification of Nickel-based Single Crystal Turbine Blades

    • Special Steel   Vol. 45, Issue 4, Pages: 34-40(2024)
    • DOI:10.20057/j.1003-8620.2024-00058    

      CLC: TG249.5
    • Received:14 March 2024,

      Published:30 July 2024

    移动端阅览

  • Sun Jiayi,Dong Longpei,Zhao Yunsong,et al.Research Progress on Numerical Simulation of Temperature Field during Directional Solidification of Nickel-based Single Crystal Turbine Blades[J].Special Steel,2024,45(04):34-40. DOI: 10.20057/j.1003-8620.2024-00058.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Thermodynamic Coupling Analysis of Air Cooling for X70 Pipeline Steel Continuous Casting Slab Based on ABAQUS
Effects of Nozzle Submerged Depth on Flow and Temperature Field of Molten Steel in Mold
Coupled Numerical Simulation of Flow Field and Temperature Field of Mold Concasting at Low Superheat by Two Rollers Cooling
Numerical Simulation of Temperature Field for GCr15 Bearing Steel Bar during Continuous Rolling Process
Computer Simulation and Analysis on Four Pass Pre-finishing Rolling Process of Steel 82B

Related Author

Fu Chengzhe
Zhang Shuai
Wang Shuang
Gao Hong
Wang Fuyue
Zhang Zherui
于会香
王万军

Related Institution

State Key Laboratory of Metal Material for Marine Equipment and Application
Ansteel Group Iron and Steel Research Institute
北京科技大学冶金与生态工程学院
太原科技大学应用科学学院
河北省科学院
0