您当前的位置:
首页 >
文章列表页 >
Effect of Aluminum Content on Microstructure and Properties of Fe-1.4C-1.5Cr-Alx Steel
Smelting and Solidification | 更新时间:2025-05-09
    • Effect of Aluminum Content on Microstructure and Properties of Fe-1.4C-1.5Cr-Alx Steel

    • Special Steel   Vol. 46, Issue 1, Pages: 54-58(2025)
    • DOI:10.20057/j.1003-8620.2024-00115    

      CLC: TG142.21
    • Received:29 April 2024,

      Published:30 January 2025

    移动端阅览

  • Shi Dafang,Yang Jun,Liu Dong,et al.Effect of Aluminum Content on Microstructure and Properties of Fe-1.4C-1.5Cr-Alx Steel[J].Special Steel,2025,46(01):54-58. DOI: 10.20057/j.1003-8620.2024-00115.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

An Analysis on Micro-Inclusion in Bearing Steel at Each Procedure of BOF-LF-VD-CC Flow Sheet
Practice of Process for Decreasing Large Size Globular Oxides Inclusion (Ds) in Bearing Steel and Gear Steel
Influence of Refining Slag on Oxygen Content and Inclusions in Bearing Steel
Quality Control of Bar Products of Bearing Steel Produced by Consteel EAF-LF(VD)-CC Process at Wuhan Iron and Steel
Simulation Analysis on Liquid Steel Flow Field in Mold with 4 Holes Immersed Nozzle and Its Application in Casting Production

Related Author

杜珊
闫绍维
王硕明
刘宪民
黄煌
刘绍康
李京社
李阳

Related Institution

河北理工大学计算机与自动控制学院
河北理工大学冶金与能源学院
石家庄钢铁有限责任公司
江阴兴澄特种钢铁有限公司花山分厂三炼钢(1),质量检验中心(2),江阴
北京科技大学冶金与生态工程学院
0