Effect of Cold Drawing Deformation and Annealing Treatment on Microstructure and Properties of GH4169 Wire
Forming and Phase Transition | 更新时间:2025-05-09
    • Effect of Cold Drawing Deformation and Annealing Treatment on Microstructure and Properties of GH4169 Wire

    • Special Steel   Vol. 46, Issue 3, Pages: 76-80(2025)
    • DOI:10.20057/j.1003-8620.2024-00125    

      CLC: TG35
    • Received:08 May 2024,

      Published:30 May 2025

    移动端阅览

  • Li Xinxu,Yu Ang,Su He,et al.Effect of Cold Drawing Deformation and Annealing Treatment on Microstructure and Properties of GH4169 Wire[J].Special Steel,2025,46(03):76-80. DOI: 10.20057/j.1003-8620.2024-00125.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Solution Heat Treatment Temperature and Cooling Mode on Microstructure and Mechanical Property of Ni-Cr-Mo-Co Alloy
Mechanical Properties of Ni-Cr-Al Alloy Cold Drawn Bar
Research Status of Ultra-low Temperature Pressure Vessel Steel
Effect of Cold-rolled Deformation on the Microstructure and Properties of GH4169 Alloy for Nuclear Power
Effects of LB/M Duplex Phase Heat Treatment on Microstructure and Mechanical Properties of Cold Working Die Steel DC53

Related Author

Fu Wangtang
Nie Yihong
Yang Xiaoyu
Wang Dapeng
Bai Xinghong
Bai Yaguan
Peng Yamin
Zhang Jiansheng

Related Institution

China First Heavy Industries
Tianjin Heavy Industries Research & Development Co., Ltd.
State Key Laboratory of Metastable Material Science and Technology, Yanshan University
Institute of Functional Materials, Central Iron and Steel Research Institute Limited
Xinyang Branch, Beijing Shouhang Science-technology Development Company
0