您当前的位置:
首页 >
文章列表页 >
Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel
Smelting and Solidification | 更新时间:2025-05-09
    • Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel

    • Special Steel   Vol. 45, Issue 6, Pages: 37-47(2024)
    • DOI:10.20057/j.1003-8620.2024-00138    

      CLC: TG142.1
    • Received:28 May 2024,

      Published:30 November 2024

    移动端阅览

  • Zheng Anmin,Fan Xuanyu,Huang Zengxin,et al.Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel[J].Special Steel,2024,45(06):37-47. DOI: 10.20057/j.1003-8620.2024-00138.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of La Treatment on Inclusions in H13 Hot Work Die Steel
Thermodynamic Simulation of Equilibrium Solidification and Precipitation of CW12MW and CW6MC Cast Nickel-based Alloys
Effect of Slag System on the Cleanliness of Electroslag Ingots during Electroslag Remelting of NiCrMoV Alloy Steel
LF Refining Slag System Optimization and Industrial Testing for 65Mn Steel
Thermodynamic Analysis of the Phase Transition of Supper Austenitic Stainless Steel S31254

Related Author

Tian Jialong
Jiang Zhouhua
Wang Lin
Jiang Chenggang
Wang Lichao
Yan Yun
Ren Ji
Su Xuehu

Related Institution

Technical Center of Fushun Special Steel Co., Ltd
School of Metallurgy, Northeastern University
Jiangsu Wanheng Casting lndustry Co., Ltd.
Division of Engineering Steel, Central Iron and Steel Research Institute
School of Metallurgical Engineering, Anhui University of Technology, Ma’anshan
0