Cause Analysis and Process Improvement Measures of Primary Forging Cracking for 20 t Flat Ingot of N08120 Nickel-based Corrosion-resistant Alloy
Product Research and Development | 更新时间:2025-05-09
    • Cause Analysis and Process Improvement Measures of Primary Forging Cracking for 20 t Flat Ingot of N08120 Nickel-based Corrosion-resistant Alloy

    • Special Steel   Vol. 46, Issue 1, Pages: 39-43(2025)
    • DOI:10.20057/j.1003-8620.2024-00141    

      CLC: TG316.2
    • Received:29 May 2024,

      Published:30 January 2025

    移动端阅览

  • Liu Yu,Xu Wenliang.Cause Analysis and Process Improvement Measures of Primary Forging Cracking for 20 t Flat Ingot of N08120 Nickel-based Corrosion-resistant Alloy[J].Special Steel,2025,46(01):39-43. DOI: 10.20057/j.1003-8620.2024-00141.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Investigation of the Law of Z Phase Precipitation Throughout the Thick Plate Production Process for N08120 Nickel-based Alloy

Related Author

Liu Yu
Xu Wenliang

Related Institution

Technical Center, Baowu Special Metallurgy Co., Ltd.
0