您当前的位置:
首页 >
文章列表页 >
Effects of Quenching and Tempering Process on Yield to Tensile Strength Ratio of S770QL High Strength Seamless Tube
Application and Service | 更新时间:2025-09-11
    • Effects of Quenching and Tempering Process on Yield to Tensile Strength Ratio of S770QL High Strength Seamless Tube

    • Special Steel   Vol. 46, Issue 5, Pages: 110-114(2025)
    • DOI:10.20057/j.1003-8620.2024-00177    

      CLC: TG156
    • Received:16 July 2024,

      Revised:2024-09-06,

      Accepted:09 September 2024,

      Published:30 September 2025

    移动端阅览

  • Du Kun,Fei Xingang,Ma Jinhui,et al.Effects of Quenching and Tempering Process on Yield to Tensile Strength Ratio of S770QL High Strength Seamless Tube[J].Special Steel,2025,46(05):110-114. DOI: 10.20057/j.1003-8620.2024-00177.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

4

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Heat Treatment Process on Structure and Properties of New Martensite Stainless Steel 6Cr15Mo for Tool
Precipitation Behavior in Tempering of Cr-W-Mo-V Semi- High Speed Steel Containing Nitrogen
Effect of Tempering on Size and Orientation of Grain in Ultra-Fine Grain Bainite Steel
Effect of Tempering Temperature on Structure and Mechanical Properties of Steel 15CrMoV Direct-Water-Quenched after Finishing Rolling

Related Author

Du Kun
聂锋
李国华
陈再枝
刘建华
马党参
邓凡宇
王明家

Related Institution

中国矿业大学(北京)
钢铁研究总院结构材料研究所
燕山大学材料学院,亚稳材料制备技术与科学重点实验室
武钢技术中心
北京科技大学高效轧制国家工程研究中心
0