任红娃,刘军利,蒋新华等.轧制工艺对410 mm×530 mm连铸坯产材等轴晶区的影响[J].特殊钢,2025,46(02):93-97.
Ren Hongwa,Liu Junli,Jiang Xinhua,et al.Influence of Rolling Process on the Equiaxed Grain Zone of Bars Produced by 410 mm × 530 mm Continuous Casting Billet[J].Special Steel,2025,46(02):93-97.
任红娃,刘军利,蒋新华等.轧制工艺对410 mm×530 mm连铸坯产材等轴晶区的影响[J].特殊钢,2025,46(02):93-97. DOI: 10.20057/j.1003-8620.2024-00178.
Ren Hongwa,Liu Junli,Jiang Xinhua,et al.Influence of Rolling Process on the Equiaxed Grain Zone of Bars Produced by 410 mm × 530 mm Continuous Casting Billet[J].Special Steel,2025,46(02):93-97. DOI: 10.20057/j.1003-8620.2024-00178.
大端面连铸坯在轧制大规格棒材时,容易出现中心疏松和缩孔、中心粗等轴晶区分布不规则等一系列内部质量问题。设计了四种不同的BD轧机(BD为英文开坯缩写,文中试验所采用的为1250双辊可逆式轧机)开坯工艺对42CrMo钢410 mm×530 mm规格的连铸坯轧制为255 mm×255 mm尺寸过程进行研究,先采用有限元模拟软件对轧制过程进行仿真模拟,再经过工业试验验证对最终
<math id="M1"><mi>ϕ</mi></math>
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=75044619&type=
2.87866688
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=75044602&type=
2.03200006
180 mm棒材成品进行低倍检验。结果表明,采用大压下量的矩形→方形→矩形交替变形机制工艺进行轧制,可有效改善产材心部疏松、缩孔缺陷,同时连铸坯心部粗等轴晶遗传至产材的尺寸接近1:1,优化产材组织对称性,便于客户后续使用。并且通过对模拟结果和工业试验检验结果对比分析显示,有限元仿真技术在轧制变形方面的应用具有较高的准确性,通过有限元仿真模拟轧制过程可有效缩短试验周期,降低工艺优化成本。
The large end face continuous casting billet is prone to a series of internal quality problems such as centre sparsity and shrinkage holes, irregular distribution of centre coarse equiaxial crystal zone when rolling large-size bars. Designed four different BD mills (BD is abbreviated for English blank, 1250 double roll reversible rolling mill used in this test) the open billet process on 42CrMo steel 410 mm × 530 mm specifications of continuous casting billet rolled to 255 mm × 255 mm size process to study, first using finite element simulation software for simulation of the rolling process, and then after the verification of industrial tests on the final
<math id="M2"><mi>ϕ</mi></math>
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=75044633&type=
2.87866688
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=75044604&type=
2.03200006
180 mm bar finished products for macrostructure test. The results show that the use of large reduction amount rectangle → square → rectangle alternating deformation mechanism process for rolling, can effectively improve the heart of the material produced loose, shrinkage defects, and at the same time, continuous casting billet heart of coarse isometric crystals inherited to the size of the material produced is close to 1:1 to optimize constructure symmetry of the material produced to facilitate the subsequent use of the customer. Moreover, the comparative analysis of the simulation results and industrial test results shows that the application of finite element simulation technology in rolling deformation has high accuracy, and the rolling process through finite element simulation can effectively shorten the test period and reduce the cost of process optimization.
陈其为 , 包汉生 , 杨 钢 , 等 . S30432钢连铸和模铸管坯的高温加工性能对比 [J]. 特殊钢 , 2023 , 44 ( 5 ): 97 - 106 .
梅德云 , 陈 敏 , 杨湘澜 , 等 . 电磁搅拌模式对大方坯结晶器内钢水流动特性的影响 [J]. 材料与冶金学报 , 2023 , 22 ( 6 ): 532 - 539 .
张越 , 吕泽安 , 马建祎 , 等 . 轻压下和拉速对42CrMo钢410 mm×530 mm铸坯轧成Φ195 mm材的低倍和中心C偏析的影响 [J]. 特殊钢 , 2021 , 42 ( 4 ): 35 - 38 .
于 莉 . Ф190 mm和Ф200 mm不锈钢棒材轧制孔型系统的优化 [J]. 特殊钢 , 2007 , 28 ( 2 ): 58 - 60 .
王敬梓 . 中碳钢高温大压下轧制流变行为及动态再结晶规律研究 [D]. 沈阳 : 东北大学 , 2017 .
王全胜 , 袁向前 . 厚板轧制过程中轧件内部变形渗透定量化研究——自主工艺设计辅助软件的探索 [J]. 宝钢技术 , 2021 ( 1 ): 14 - 18 .
赵景存 , 李 雷 , 朱 叶 . 22CrMoH钢轧制过程中金属流变对锭型偏析的影响 [J]. 河北冶金 , 2021 ( 10 ): 33 - 36 .
赵博志 , 邓加东 , 钱东升 , 等 . 面向大型环件径轴向稳定高效轧制的变形过程规划方法研究 [J]. 塑性工程学报 , 2023 , 30 ( 9 ): 9 - 16 .
赵 杰 , 赵景存 . 轧制对锭型偏析的影响 [J]. 山西冶金 , 2021 , 44 ( 5 ): 26 - 28 .
吴晨辉 , 吴国荣 , 张 敏 , 等 . 板坯连铸过程热收缩变形行为研究 [J]. 钢铁钒钛 , 2023 , 44 ( 2 ): 141 - 146 .
史海军 . 特厚板变厚度轧制过程金属流动规律研究 [D]. 沈阳 : 东北大学 , 2019 .
石可伟 , 张洪才 , 郑力宁 , 等 . 齿轮钢大圆坯的铸态组织及轧制遗传性 [J]. 连铸 , 2020 , 45 ( 4 ): 66 - 69 .
孙 涛 , 岳 峰 , 林 寒 , 等 . 大断面圆坯凝固组织及力学性能分析 [J]. 炼钢 , 2016 , 32 ( 1 ): 66 - 69 .
0
Views
1
下载量
0
CSCD
0
CNKI被引量
Publicity Resources
Related Articles
Related Author
Related Institution
京公网安备11010802024621