Development of a New Type L80 Grade 13Cr Martensitic Oil Well Pipe
Product Research and Development | 更新时间:2025-11-06
    • Development of a New Type L80 Grade 13Cr Martensitic Oil Well Pipe

    • Special Steel   Vol. 46, Issue 6, Pages: 90-94(2025)
    • DOI:10.20057/j.1003-8620.2024-00199    

      CLC: TG113.23
    • Received:09 August 2024,

      Revised:2024-10-18,

      Accepted:21 October 2024,

      Published:30 November 2025

    移动端阅览

  • Peng Jun,Li Danyang,Ding Lei,et al.Development of a New Type L80 Grade 13Cr Martensitic Oil Well Pipe[J].Special Steel,2025,46(06):90-94. DOI: 10.20057/j.1003-8620.2024-00199.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

4

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Current Situation and Prospects of Resource Application of CO2 in Steelmaking Process

Related Author

Peng Jun
Peng Feng
Li Xiao
Deng Haohua

Related Institution

China Metallurgical Industry Planning and Research Institute
0