Effect Mechanism of Curling Temperature on the Toughness of Titanium Microalloyed High-strength Steel GCL700
Forming and Phase Transition | 更新时间:2025-05-09
    • Effect Mechanism of Curling Temperature on the Toughness of Titanium Microalloyed High-strength Steel GCL700

    • Special Steel   Vol. 46, Issue 3, Pages: 66-75(2025)
    • DOI:10.20057/j.1003-8620.2024-00231    

      CLC: TG161
    • Received:23 September 2024,

      Published:30 May 2025

    移动端阅览

  • Wang Yi,Che Zhichao,Chen Yufeng,et al.Effect Mechanism of Curling Temperature on the Toughness of Titanium Microalloyed High-strength Steel GCL700[J].Special Steel,2025,46(03):66-75. DOI: 10.20057/j.1003-8620.2024-00231.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effects of Ti Microalloying on the Microstructure and Mechanical Properties of a Novel GH1059 Alloy for Nuclear Applications
Effect of Nioblum on Microstructure and Properties of 65Mn High Carbon Cutting Tool Steel
Impact of the Annealing Temperature on the Magnetic and Mechanical Characteristics of Thin-gauge Non-oriented Electrical Steel
Effects of Solution Temperature on Microstructure and Tensile Properties of a Novel Ni-Co-Based Wrought Superalloy
Effect of Heat Treatment Temperature on Microstructure and Properties of Fe-27Mn-9Al-1C-0.25V Low-density Steel

Related Author

Yao Zhiqiang
Wu Jinrong
Guan Xianjun
Wu Yunsheng
Qin Xuezhi
Zhou Lanzhang
Wang Jiaqi
Zhao Le

Related Institution

State Key Laboratory of Advanced Marine Materials, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences
CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences
School of Materials Science and Engineering, University of Science and Technology of China
changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences
School of Materials Science and Engineering, Dalian University of Technology Liaoning
0