Practical Application of Dispersion Breathable Brick in 70 t Refining Ladle
Smelting and Solidification | 更新时间:2026-01-16
    • Practical Application of Dispersion Breathable Brick in 70 t Refining Ladle

    • Special Steel   Vol. 47, Issue 1, Pages: 78-82(2026)
    • DOI:10.20057/j.1003-8620.2024-00242    

      CLC: TF702+.9
    • Received:10 October 2024,

      Published:30 January 2026

    移动端阅览

  • Huang Guotao,Wei Shangjin,Li Bo,et al.Practical Application of Dispersion Breathable Brick in 70 t Refining Ladle[J].Special Steel,2026,47(01):78-82. DOI: 10.20057/j.1003-8620.2024-00242.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

86

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Different Residual Steel Amounts on Molten Steel Cleanliness
Effect on Fatigue Failure Behavior Induced by Inclusions in GCr15 Bearing Steel Under Different Metallurgical Processes
Process Practice of a 90 t Ladle Wire Feeding
Finite Element Simulation of Stable State Temperature Field of Ladle
Phased Optimization Process for Shaft Electric Arc Furnace Smelting with High Hot Metal Ratio

Related Author

Huang Guotao
Zhang Lifeng
Zhang Hejun
Lu Boxun
Wang Bochen
Liu Zhonghua
Ren Ying
Luo Haiwen

Related Institution

School of Mechanical and Materials Engineering, North China University of Technology
Tangshan Iron and Steel Group Co., Ltd., Steelmaking Division
Tangshan Iron and Steel Group Co., Ltd., Research and Development Center
Metallurgical Corporation of China (MCC) CADI Ironmaking Division
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing
0