Technology for Controlling Nitrogen Content in Molten Steel Melted by 120-ton Top-bottom Reblowing Converter
Smelting and Solidification | 更新时间:2025-09-11
    • Technology for Controlling Nitrogen Content in Molten Steel Melted by 120-ton Top-bottom Reblowing Converter

    • Special Steel   Vol. 46, Issue 5, Pages: 24-31(2025)
    • DOI:10.20057/j.1003-8620.2025-00037    

      CLC: TF704.6
    • Received:15 February 2025,

      Revised:2025-04-14,

      Accepted:21 April 2025,

      Published:30 September 2025

    移动端阅览

  • Cao Shuwei,Song Wanping,Chen Yu.Technology for Controlling Nitrogen Content in Molten Steel Melted by 120-ton Top-bottom Reblowing Converter[J].Special Steel,2025,46(05):24-31. DOI: 10.20057/j.1003-8620.2025-00037.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

4

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Smelting Process Practice to Improve the Cleanliness and Polishling Proptice of Die Steel
Process Analysis and Experiment of Precise Control of Nitrogen Content in Pressure Smelting of Mn18Cr18N
Effect of Nitrogen Content and Final Rolling Temperature on Low-temperature Impact Toughness of Titanium Microalloyed High-strength Steel CGLC700
Research on the Production Practice of 09CuPCrNi Weather Resistant Steel

Related Author

Cao Shuwei
Song Wanping
Tian Zhiqiang
Fan Mingqiang
Zhao Zhengrong
Zhao Nan
Zhao YingLi
LiuYong

Related Institution

Special Materials Research and Development Center,Material Technology Research Institute of HBIS Group
Department of Metallurgical Technology Research, Central Iron and Steel Research Institute;Co., Ltd.
Material Digital Research and Development Center,China Iron and Steel Research Institute Group
School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
Chengde Branch, HBIS Group Co., Ltd.
0