Effect of Heat Treatment Process on the Section Shrinkage of 1Cr16Ni2MoN Blade Steel
Application and Service | 更新时间:2025-09-02
    • Effect of Heat Treatment Process on the Section Shrinkage of 1Cr16Ni2MoN Blade Steel

    • Special Steel   Vol. 46, Issue 4, Pages: 163-168(2025)
    • DOI:10.20057/j.1003-8620.2025-00060    

      CLC: TG156.3
    • Received:07 March 2025,

      Revised:2025-05-08,

      Accepted:08 May 2025,

      Published:30 July 2025

    移动端阅览

  • Zhang Xiuli,Gong Zhihua,Liu Xinquan,et al.Effect of Heat Treatment Process on the Section Shrinkage of 1Cr16Ni2MoN Blade Steel[J].Special Steel,2025,46(04):163-168. DOI: 10.20057/j.1003-8620.2025-00060.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0