您当前的位置:
首页 >
文章列表页 >
Influence of Phosphorus Microalloying on Molidification, Hot Deformation and Mechanical Properties in Nickel/Nickel Iron-based Alloys
Overview | 更新时间:2025-09-02
    • Influence of Phosphorus Microalloying on Molidification, Hot Deformation and Mechanical Properties in Nickel/Nickel Iron-based Alloys

    • Special Steel   Vol. 46, Issue 4, Pages: 12-23(2025)
    • DOI:10.20057/j.1003-8620.2025-00101    

      CLC: TG146.1
    • Received:16 April 2025,

      Revised:2025-05-17,

      Accepted:20 May 2025,

      Published:30 July 2025

    移动端阅览

  • Wang Changshuai,Wu Yunsheng,Wu Hao,et al.Influence of Phosphorus Microalloying on Molidification, Hot Deformation and Mechanical Properties in Nickel/Nickel Iron-based Alloys[J].Special Steel,2025,46(04):12-23. DOI: 10.20057/j.1003-8620.2025-00101.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

1

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Heat Treatment on Mechanical Properties of High Strength Free-Cutting Precipitation Hardening Stainless Steel 2Cr16Ni3Mo2CuN
Effect of Quenching and Tempering Process on Mechanical Properties of Spring Steel 60Si2CrVAT
Structure and Mechanical Properties of Linepipe Steel X80
Structure and Properties of a Ti-IF Steel Hot-Rolled in Ferrite Region
Production Practice of Steel 37CrMnMo for Coupling Sleeve of Petroleum Drill Stem

Related Author

李志
高谦
高登攀
江志华
姜洪胜
许广鹏
李英
聂爱诚

Related Institution

江阴兴澄特种钢铁有限公司,江阴
中国石油天然气集团公司管材研究所
中原工学院材料与化学工程系
西安交通大学材料科学与工程学院
西安石油大学
0