Effect of Aging Temperature on Mechanical Properties of Martensite Precipitation Hardening Stainless Steel0Cr15Ni5WMoVNb
#br#

Guo yanfeil1,2, Yang Zhouyue2, Ding Yali2, Liu Zhiyong1, Chen Jiayan2   

  1. 1 Key Lab of Materials Physics, Ministry of Education, School of Physical Science and Engineering, Zhengzhou University, Zhengzhou 450052;
    2 Institute for Structure Materials, Iron & Steel Research Institute, Beijing 100081
  • Received:2010-02-25 Published:2010-08-01 Online:2022-11-20

摘要: 0Cr15Ni5WMoVNb钢(%:0.068C、14.54Cr、5.32Ni、0.88W、0.92Mo、0.20V、0.10Nb)经5 t中频感应炉+2 t真空电渣重熔炉冶炼,经锻造、热轧成Φ45 mm棒材,试样经1 000℃30 min固溶空冷+-70℃2 h冷处理后进行400~600℃4 h时效空冷。试验结果表明,在450℃时效0Cr15Ni5WMoVNb钢的强度最大,以准解理断裂为主,冲击功低为40 J,随时效温度上升,冲击功显著上升,强度下降,在510℃时效该钢有良好的强韧性,抗拉强度Rm 1300 MPa,屈服强度Rp0.21100 MPa,冲击能AKV 100 J。

Abstract: The studied steel 0Cr15Ni5WMoVNb(%:0.068C,14.54Cr,5.32Ni,0.88W,0.92Mo,0.20V, 0. 10Nb)is  melted by  5  t  medium  frequency  induction  furnace+2  t  vacuum  electro-slag  remelting  furnace,then  forged  and hot  rolled  to  φ45  mm  bar  products,and  the  test  specimens  solid-solution-treated  at  1000  ℃  for  30  min  +cold-treated  at -70℃  for  2  h  are  aged  at  400~600  ℃  for4  h.  Test  results  show  that  with  aging  at  450  ℃,the  strength  of  steel 0Cr15Ni5WMoVNb is up to maximum value with main quasi-cleavage fracture and low impact energy-40J,with increasing aging temperature the impact energy of steel increases obviously and strength decreases,and with aging at 510 ℃ the steel has  excellent  strength-toughness  i.e.tensile  strengh  Rm  1300  MPa,yield  strength  Ro.21100  MPa  and  impact  energy  Akv 100 J.