ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2010, Vol. 31 ›› Issue (4): 68-70.

• 组织和性能 • 上一篇    

碳含量对贝氏体型冷作强化非调质钢的组织和力学性能的影响

计芳芳1,2,  惠卫军1,2, 吴勇生1, 于同仁3,  孙  维3   

  1. 1昆明理工大学材料科学与工程学院,昆明650093;
    2钢铁研究总院先进钢铁材料技术国家工程研究中心,北京100081; 3马鞍山钢铁股份有限公司技术中心,马鞍山243002
  • 收稿日期:2010-03-03 出版日期:2010-08-01 发布日期:2022-11-21
  • 通讯作者: 通讯作者:吴勇生,教授,昆明理工大学材料科学与工程学院,昆明650093
  • 作者简介:计芳芳(1984-),女,硕士研究生,贝氏体型冷作强化非调质钢的组织和力学性能研究。
  • 基金资助:
    国家科技支撑计划资助项目(2007BAE30BO4)

Effect of Carbon Content on Structure and Mechanical Properties of Cold Hardening Micro alloyed Bainite Steel

Ji Fangfang1,2, HuiWeijun1,2, Wu Yongsheng1, Yu Tongren3, Sun Wei3   

  1. 1 Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093.
    2 National Engineering Research Center of Advanced Steel Technology, Central Iron and Steel Research Institute, Beijing    100081.
    3 Technical Center, Maanshan Iron and Steel Co Ltd, Maanshan    243002
  • Received:2010-03-03 Published:2010-08-01 Online:2022-11-21

摘要: 研究了0.09%~0.14%C含量对5%~50%冷拔减面率和100~500℃2 h时效处理的2Mn-0.003B-0.05Ti非调质钢组织和力学性能的影响。结果表明,当碳含量较低(0.09%~0.12%C)时,可获得比较细小均匀的粒状贝氏体组织,但当碳含量为0.14%时,则组织中出现块状铁素体;在相同的拉拔减面率下,随着碳含量的增加,该钢的强度提高,塑性降低,当减面率较大时,这种差别比较明显;随着碳含量的升高,时效处理后的该钢强度增量明显降低。

关键词:  Mn-B-Ti冷作强化非调质钢, 碳含量, , 粒状贝氏体, 力学性能

Abstract: Effect    of   0.09%~0. 14%    C    content    on    structure    and    mechanical    properties    of   2Mn-0.003B-0.05Ti    micro- alloying   steel   cold   drawn   with   5%~50%   reduction   and   aged   at   100~500   ℃   for   2   h   has   been   studied.   Results   show   that with    lower    carbon    content (0.09%~0. 12%C), the    finer    and    uniform    distributed    granular    bainite    structure    in    steel    is    obtained, while    with    0. 14%    C, the    lumpy    ferrite    shall    occur    in    structure; at    same    cold-drawing    reduction, with    increasing carbon   content   the   strength   of   steel   increases   and   plasticity   decreases, and   the   larger   the   reduction, the   more   significant   the tendency; and   with   increasing   carbon   content   the   increment   of   strength   of   steel   aged   obviously   decreases.

Key words:  , Mn-B-Ti Cold-Hardening Microalloying Steel, Carbon Content, Granular Bainite, Mechanical Properties