摘要: 研究了固溶温度750~1050℃对00Ni14Cr3Mo3Ti新型马氏体时效钢冲击性能和硬度的影响,并用扫描电镜观察试验钢冲击断口的形貌和固溶态显微组织。试验结果表明,钢的固溶温度低于900℃时,随着固溶温度的升高,基体中未溶的Laves相逐渐溶解,固溶态和510℃ 5 h时效态的冲击性能均随着固溶温度的上升而提高;固溶温度高于900℃,固溶态冲击性能随着固溶温度的上升而提高,该钢固溶态冲击功由900℃的215J增加至1050℃固溶的226J,但时效态冲击性能随着固溶温度上升而降低,510 5h时效钢的冲击功由900℃最大值62J降至1050℃固溶的25J。
[1] Haynes A G, Development and Future Potential of Maraging Steels [J]. Journal of the Royal Aeronautical Society, 1966,70 :766-772.
[2] He Y, Yang K,et al. Effects of Solution Treatment Temperature on Grain Growth and Mechanical Properties of High Strength 18% Ni Cobalt Free Maraging Steel [J]. Materials Science and Technology, 2003,19(2) : 117-124.
[3] Tarasenko L V, Zvigintsev N V and Titov V I, et al. Structure and Composition of Intermetallic Phases and Properties of Steel 00KhllN10M2T [ J ]. Fizika Metallovi Metallovedenie, 1985, 59 (3) :551-558.
[4](美)查利oR.布鲁克斯(CharUe R. Brooks),(美)阿肖克。考霍 莱(Ashok Choudhury)著;谢斐娟,孙家骤,译.工程材料的失效 分析[M].北京:机械工业出版社,2003 : 123-134.
[5]杨维宇,丁雅莉,杨卓越,等.固溶温度对马氏体时效钢 00Nil4Cr3Mo3Ti组织和力学性能的影响[J].特殊钢,2009,30 (3):61-62.
[6]Rack H J and Holloway P H. Grain Boundary Precipitation in 18Ni Maraging Steels[J]. Metallurgical Transactions11977,8A(8) :1313-1315.
[7]Rack H J and Kalish D. Strength and Fracture Toughness of 18Ni (350) Maraging Steel [J]. Metallurgical Transactions, 1971,2A (11):3011-3020.
[8]高晓婷,任卫斌,赵金龙,等.固溶温度对18NiC250材料力学性能的影响[J].热加工工艺,2018,47(6):198-200.
任艳茹, 刘周利, 杨维宇, 赵卫东. 固溶温度对新型无钻马氏体时效钢00Nil4Cr3Mo3Ti 冲击性能的影响[J]. 特殊钢, 2020, 41(1): 64-67.
Ren Yanni , Liu Zhouli, Yang Weiyu , Zhao Weidong. Effect of Solution Temperature on Impact Property of New Co-free Maraging Steel 00Nil4Cr3Mo3Ti[J]. Special Steel, 2020, 41(1): 64-67.