Operational Practice of Heel Slag + Single Slag for Steelmaking High Carbon Steel in 100 t BOF with Titanium-Bearing Hot Metal

Zhai Yongqiang1 ,Wang Jianwei1,Zhang Yi1 ,Xia Chaokai1 , Wang Linsong1 ,Gao Changyi2   

  1. 1 Shuicheng Iron and Steel Group Corp, Liupanshui 553028 ;
    2 Manufacture Management Department, Shuicheng Iron and Steel Group Coip, Liupanshui 553028
  • Received:2020-04-20 Online:2020-10-01 Published:2022-05-05

100t转炉用含钛铁水冶炼高碳钢的留渣+单渣操作实践

翟勇强1, 王建伟1,张 毅1,夏朝开1,王琳松1,高长益2   

  1. 1水城钢铁集团公司,六盘水5530281
    2水城钢铁集团公司制造管理部,六盘水553028
  • 作者简介:翟勇强(1968 -),男,硕士 ( 2006年武汉科技大学),1991年 贵州工学院(本科)毕业,髙级工程师,钢铁冶金技术研究。

Abstract: Aiming at the problems such as difficult melting of slag and low dephosphorization rate at the early stage of steelmaking high carbon steel in 100 t BOF ( basic oxygen furnace) with titanium-bearing hot metal, the slagging process and the slag physical characters of BOF steelmaking with titanium-bearing hot metal are analyzed, the technology of heel slag + single slag is developed,:, e. The terminal slag is recycled to use,to full play the character of high FeO content of 10% 〜13% FeO in the terminal slag, the CaO-TiO2-SiO2 ternaiy slag system in the early stage of steelmaking of titanium-bearing hot metal is rapidly converted into the Ca0-TiO2 -SiO2 -FeO quaternary slag system, so that most of phosphorus in steel is removed. The basicity of terminal slag is controlled to be more than 3. 2 , the TiO2 content in terminal slag is controlled to be less than 5% ,the BOF tapping [C]≥0.20% and tapping [P]≤0.014%  , the dephosphorization rate of steelmaking in BOF reaches to 88% 〜92% ,and the consumption of lime decreases to 28 kg per ton of steel.

Key words:  , 100 t BOF, Titanium-Bearing Hot Metal, High Carbon Steel, Slag Heel Operation, Single-Slag Operation

摘要: 针对100t转炉用含钛铁水冶炼高碳钢的前期成渣难于熔化、脱磷率低的问题,分析了含钛铁水转炉炼钢的成渣过程和炉渣的物理特性,开发了留渣+单渣工艺技术。循环利用终点炉渣,充分发挥渣中10%~13%FeO高(FeO)含量的特点,快速把含钛铁水冶炼前期的CaO-TiO2-SiO2三元渣系转变为CaO-TiO2-SiO2-FeO四元渣系,脱除钢中大部分磷。控制终渣碱度大于3.2、(TiO2)含量小于5%,使转炉出钢[C]≥0.20%、[P]≤0.014%,转炉炼钢脱磷率达到88%~92%,石灰消耗下降到28 kg/t钢。