Research and Development of Hot Rolled Strip of  BTQ001 Oriented Silicon Steel

Lu Xiaoyu, Wang Shaobing, Huang Li , Dong Lili   

  1. Technology Center of Steel Union Co. Ltd. of Baotou Steel (Group) Corp. , Baotou 014010
  • Received:2020-04-28 Online:2020-10-01 Published:2022-05-05

取向硅钢热轧钢带BTQ001研制与开发

卢晓禹,王少炳,黄利,董丽丽   

  1. 包钢钢联股份有限公司技术中心,包头014010
  • 作者简介:卢晓禹(1985-),男,硕士(内蒙古科技大学),高级工程师, 河北工业大学(本科)毕业,金属材料研究。

Abstract: The production flowsheet of BTQ001 steel is 230 mm cast slab-2.3 mm hot rolled plate-0.63 mm first cold rolled sheet-850 °C annealing-0. 27 mm second cold rolled sheet-1200°C annealing, the changes of microstructure of the products in each phase are analyzed, and the magnetic properties of the finished products of oriented silicon steel are statistically analyzed. The experimental results show that the BTQ001 oriented silicon steel optimum production process is to control the heating temperature at 1280 ~ 1300 °C for hot rolling, the finishing rolling at 950 °C and coiling at 550 °C.

摘要: BTQ001钢的生产流程为230 mm铸坯-2.3 mm热轧板-0.63 mm一次冷轧板-850℃退火-0.27 mm二次冷轧板-1200℃退火,分析各阶段产品显微组织的变化,同时对取向硅钢成品磁性能进行统计。试验研究结果表明,BTQ001取向硅钢热轧加热温度为1280~1300℃,精轧终轧温度控制在950℃、卷取温度为550℃为最佳生产工艺