ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2019, Vol. 40 ›› Issue (3): 23-27.

Previous Articles     Next Articles

Development and Application of Deep Drawing Hot-Rolled Steel  for Enameling Water Tank

Liu Yourong1 , Sun Quanshe2   

  1. 1 R&D Center for Meisteel, Baosteel Research Institute, Nanjing 210039 ;
    2 Research Center Institute, Baosteel Co. Ltd. , Shanghai 201900
  • Received:2019-11-12 Online:2019-06-01 Published:2022-05-16

深拉型搪瓷内胆用热轧钢带开发及应用

刘友荣1,孙全社2   

  1. 1宝钢股份研究院梅钢公司技术中心,南京210039;
    2宝山钢铁股份有限公司中央研究院,上海201900
  • 作者简介:刘友荣(1969-),男,硕士(2007年安徽工业大学),高级主任研究员,1995年西安建筑科技大学(本科)毕业,热轧板带产品开发。

Abstract: The structure of enameling water tank is upgraded from three-segment type to two-segment type. The manufacturing process of water tank is changed from sheet curling and stamping craft to the sheet deep drawing craft. Because of the structure change of water tank, there are much more requirements on enameling property and formability for steel sheet. Baosteel industrial data and Design of Experiments ( DOE) method are used to establish the steel designing and optimizing model, and the special deep drawing hot-rolled steel for enameling water tank is developed successfully. It has been proved by large industrial production that, the reject ratio of deep drawing parts can be controlled down the level of 0. 4% , at the same time, the enameling property is excellent.

摘要: 热水器搪瓷内胆结构由三段式升级为二段式,内胆毛坯的成形方式由卷圆成形+冲压成形方式转变成深拉成形方式,相应的钢板也必须满足深拉成形要求。由于搪瓷内胆结构的变化,对钢板提出了更高的要求,在保障涂搪性能的基础上还需更好的深拉性能。宝钢运用钢厂工业数据与试验设计(DOE)工具,建立钢种设计优化模型,开发出了深拉型搪瓷内胆专用热轧钢板。经工业大生产验证,深拉件报废比例可以控制在千分之四以内,涂搪性能优良。