Abstract: Based on analogy theory,1:4 water model has been established for 300 t RH refining unit at Masteel The effects of different immersion depth on circulation flow, mixing time and residence time of vacuum chamber were investigated. Test results show that the circulating flow rate increases with the increase of immersion depth. When the immersion depth is greater than 500 mm, the upward trend of circulating flow slows down. When immersion depth is greater than 500 mm,the mixing time is low. When the immersion depth reaches 520 mm,the rising trend of the residence time of the vacuum chamber begins to weaken. When the immersion depth exceeds 560 mm,the residence time of the vacuum chamber changes little. Taking account of the above factors, the optimum immersion depth of 300 t RH at Masteel should be controlled within 520 ~ 560 mm.
摘要: 基于相似原理,按照1:4的比例对马钢300 tRH精炼装置建立了水模型,考察了不同浸渍管浸入深度对循环流量、混匀时间、真空室内停留时间等参数的影响。试验结果表明,随着浸入深度的增加,循环流量呈上升趋势,当浸渍管浸入深度大于500 mm时,循环流量上升趋势减缓;浸渍管浸入深度大于500 mm时,混匀时间出现低点;当浸入深度到达520 mm时,真空室停留时间上升趋势开始减弱,当浸入深度超过560 mm后,真空室停留时间变化较小。综合考虑以上因素,马钢300 t RH最佳的浸渍管浸入深度应控制在520~560 mm内。
Li Yingjiang. Experimental Study on Impregnation Depth of Immersion Tubes in 300 t RH Refining Unit[J]. Special Steel, 2019, 40(2): 1-4.
李应江. 300 t RH精炼装置浸渍管浸入深度的试验研究[J]. 特殊钢, 2019, 40(2): 1-4.