Development of 29MnCr6 Steel for L80-1 Grade High Anti-Crushing Oil Casing Tube

Cheng kai1 ,Feng Ying1,2, Deng Xuyan1,2 ,Liu Ke1,2 , Li Yingzhen1,2   

  1. 1 R&D Center,Dalipal Pipe Co,Cangzhou 061000;
    2 HeBei OCTG Engineering Technology Research Center, Cangzhou 061000
  • Received:2018-09-15 Online:2019-04-01 Published:2022-05-18

L80-1级高抗挤毁石油套管用钢29MnCr6的开发

程凯1, 冯莹冷1,2, 邓叙燕1,2, 刘珂1,2, 李英真1,2   

  1. 1达力普石油专用管有限公司技术中心沧州061000;
    2河北省石油专用管工程技术研究中心沧州061000
  • 作者简介:程凯(1991-)男,硕士(2017年河北工程大学),助理工程师,2014年河北工程大学(本科)毕业,无缝钢管轧制工艺设计。

Abstract: The economy material of 29MnCr6 was developed successfully by dalipia pipe company, which to product collapse resistance oil casing tube of Φ244. 5 mm x 10. 03 mm specification L80-1 grade. Compare with the conventional 25CrMo material ,29MnCi6 material has the characteristics of low smelting cost and low heat treatment energy consumption, which can reduce production cost. By actual performance testing, compared with the conventional 25CrMo material, the L80- 1 steel grade oil casing that 29MnCr6 material producted has same tensile properties basically, the impact toughness meets APT 5 CT standard requirement, and the collapse resistance values are similar, bose have high level of collapsehigher that higher API Bull 5C2 collapse resistance standard value 60% , but meets the requirements of API 5 CT standard fully. So 29MnCr6 material can instead of 25CrMo material completely.

Key words:  , Economy, Oil Casing Tube, High Resistance to Collapse, L80 Grade ,

摘要: 达力普石油专用管有限公司成功开发出用于生产Φ244.5 mm×10. 03 mm规格L80-1钢级抗挤毁石油套管的经济性材质-29MnCr6。与常规25CrMo材质相比,29MnCr6材质冶炼成本低,热处理能耗小,可降低生产成本。经性能检测,29MnCi6材质与常规25CrMo材质相比,轧制出的L80-1钢级石油套管拉伸性能相当,冲击韧性符合API 5CT标准要求,而且抗挤毁值相差不大,均具有高出API Bull 5C2标准抗挤毁值60%的高抗挤毁水平,因此,29MnCr6材质完全可代替25CrMo材质。