Abstract: This research investigated 8.0 mm thick high strength weathering steel Q550NQR1 with relatively low -40℃ low temperature impact value, and multiple pearlite segregation bands were observed in core microstructure, although the segregation bands are narrow and discrete, the quantity is numerous and ratio reaches 5. 8% ; through test, the segregation band in core microstructure has little effects on mechanical performance of tested steel, which is considered to be resulted from the effects of fine grain strengthening and precipitation strengthening by Nb-V micro alloying; however, the interface of ferrite and pearlite is relatively weak, which facilitates generation and extension of crack, as well as the pearlite segregation band likely leads to increase of ductile-brittle transition temperature thereby deteriorating low temperature impact toughness of tested steel. The improved technologies that increasing heating temperature and assuring enough heating time, increasing cooling rate in laminar cooling section as well as controlling the contents of Nb and V were adopted to conduct rolling, and for the final product, grain refinement achieves, pearlite segregation band vanishes, mechanical performance satisfies requirement and the surplus is appropriate, as well as -40℃low temperature impact average value increases 84.3 J.
摘要: 研究分析了8.0 mm厚Q550NQR1高强耐候钢-40℃低温冲击功偏低的原因,于其心部组织观察到多条珠光体偏析带,该偏析带虽宽度窄,且较分散、不连续,但是数量多,占比约5.8%;经检测,该心部偏析对试验钢力学性能影响不大,认为主要是铌钒微合金化的细晶强化和析出强化效果,保证了试验钢的高强度;然而,铁素体/珠光体的界面相对薄弱,利于裂纹的产生和扩展,并且珠光体偏析带可能使材料的韧脆转变温度升高,从而使得试验钢的低温冲击韧性变差。通过提高加热温度并保证足够的加热时间、提高层流冷却段冷却速度、控制Nb和V含量的改进工艺进行轧制,所得产品组织细化、珠光体偏析带消失、常规力学性能符合要求,且富余量合适、-40℃低温冲击值均值上升84.3 J。
关键词: 高强耐候钢Q550NQR1, 珠光体偏析, -40℃, 冲击韧性, 铌, 钒
Cui Kaiyu. Technology Practice of Increasing Impact Engergy of Weathering Steel Q550NQR1 at -40℃[J]. Special Steel, 2018, 39(5): 54-57.
崔凯禹. 提高Q550NQR1耐候钢-40℃冲击功的工艺实践[J]. 特殊钢, 2018, 39(5): 54-57.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2018/V39/I5/54