[1] |
Zhang Xingli, Qi Fengyou, Su Yongze, Cui Guibo, Tang Qing, Hou Jianwei.
Ractice of EF3 Ultra-low Phosphorus Smelting Process for High-grade Pipeline Welding Wire
[J]. Special Steel, 2024, 45(6): 57-61.
|
[2] |
Cao Xiaoqiang, Jia Jianwen , Yue Xiwen, Hu Qunkun , Wei Yinghui , Hou Lifeng.
High Temperature Oxidation Behavior of S44535 Ferritic Stainless Steel
[J]. Special Steel, 2024, 45(2): 66-73.
|
[3] |
Qin Mozhou, Zhao Guangdi, Wu Jinjiang, Zhao Yuanyuan, Wang Guoan.
Isothermal Oxidation Behavior of Nickel-based Superalloy U720Li in Different Oxidation Stages at 750 ℃
[J]. Special Steel, 2024, 45(1): 12-17.
|
[4] |
Zhang Tianshu, Huang Zhicheng, Chi Yunguang, Yang Jian.
Steelmaking Production Practice of 9Ni Steel for Ulta-low Temperature Pressure Vessel
[J]. Special Steel, 2024, 45(1): 27-32.
|
[5] |
Huang Gaojian, Wei Zehong, Song Huan, Zhan Dongping, Geng Bin, Yang Yongkun.
Practice of Economical Smelting of Q355 Steel in Converter
[J]. Special Steel, 2024, 45(1): 70-76.
|
[6] |
Peng Leizhen, Jiang Zhouhua, Shen Guoqu, Geng Xin, Qiu Guoxing, Wang Cheng.
Oxidation Behavior of Electrode Surface and Deoxidation System During Electroslag Remelting 9CrMoCoB Steel
[J]. Special Steel, 2023, 44(6): 70-77.
|
[7] |
Zhang Fudong, Wu Bo, Wang Yuecong, Zhao Xin, Liang Chao.
The Smelting Process Improvement of 120 t Top-Bottom Combined Blown Converter with High-Carbon Turndown and Low Phosphorus Tapping
[J]. Special Steel, 2023, 44(6): 63-69.
|
[8] |
Li Likai, Gao Fang, Wang Min, He Xiaoyu, Li Yihong, Bao Yanping.
The Effect of Scrap Ratio on the Peroxidation of Molten Steel in Converter and the Optimization of Ingredient
[J]. Special Steel, 2023, 44(3): 39-45.
|
[9] |
Zhao Bin , Zhang Na , Peng Guohong , Wang Chengyi , Wu Wei , Wu Wei.
Experimental Study on Dephosphorization of X80 Pipeline Steel by Duplex Steelmaking Technology for Combined Blowing Converter
[J]. Special Steel, 2023, 44(2): 52-55.
|
[10] |
Zhang Xin wen , Shi Jiakai , Wang Dewei , Xuan Kangle , Liu Yong , Meng Xiangyan.
Comparison and Analysis of Secondary Oxidation Degree in the First Heat of Continuous Casting
[J]. Special Steel, 2023, 44(2): 56-60.
|
[11] |
Zeng Li , Wang Bin , Xu Mei , Zhang Wei.
Effect Mechanism of Boron on High Temperature Oxidation Properties of Austenitic Stainless Steel
[J]. Special Steel, 2023, 44(2): 61-64.
|
[12] |
Yang Limei , Yin Chuanlei , Ma Qingfeng , Zhai Wanli , Liu Congde , Zuo Hui.
Production Practice of 90 t BOF⁃RH⁃CC Process for ZG⁃12 Ultra⁃low Phosphorus Steel
[J]. Special Steel, 2023, 44(1): 15-18.
|
[13] |
Chen Junzhao, Zhang Yanhui , Tan Antong , Li Likai, Kang Jianguang.
Application of Particle Injection Dephosphorization Process on Steelmaking of 130 t Electric Arc Furnace
[J]. Special Steel, 2023, 44(1): 34-38.
|
[14] |
Xiao Bingzheng , Xie Haiping , Wei Gangwu , Sun Taoan, Wang Haichuan, Deng Aijun.
Optimization of “C-P-T” Co-operating Control Process in Converter Steelmaking for GCr15 Bearing Steel
[J]. Special Steel, 2022, 43(6): 54-59.
|
[15] |
Wang Zhongliang, Bao Yanping, Gu Chao, Liu Yu, Huang Yongsheng.
Control of Ds Inclusions in GCr15 Bearing Steel Based on Non-aluminum Deoxidation Process
[J]. Special Steel, 2022, 43(6): 8-12.
|