Abstract: The production flowsheet of steel FAS2225 (/%: 0.26C, 0.35Si, 1.99Mn, 0.013P, 0.046S, 0.54Cr, 0.12V, 0.02Mo, 0.08Ni, 0.0012O, 0.0070N) is pretreated hot-metal-60t top and bottom combined brown converter- LF-VD-300mmx360mm bloom casting-continuous rolling. The hole formed by center crack of 215mmx213mm rolled billet occurs. And it is obtained by analysis that the thermal stress and structure stress produced by larger heating speed and temperature gradient of casting bloom lead to cracks of bloom and forming hole-cracks of billet during rolling process. By decreasing the heating temperature of bloom at preheating zone in heating furnace from 900℃ to 750℃, prolonging heating time and decreasing temperature gradient from △200℃ to △100℃, it is available to inhibit the formation of hole-defects.
摘要: FAS2225钢(/%:0.26C,0.35Si,1.99Mn,0.013P,0.046S,0.54Cr,0.12V,0.02Mo,0.08Ni,0.0012O,0.0070N)的生产流程为铁水预处理-60t顶底复吹转炉-LF-VD-300mm×360mm坯连铸-连轧。在215mm×213mm轧坯上出现中心开裂形成孔洞。经分析得出,加热速度过快及温度梯度过大产生的热应力和组织应力使连铸坯发生开裂造成轧制过程孔洞缺陷。通过预热段加热温度从900℃降至750℃,延长加热时间、温度梯度从△200℃降至△100℃有效遏制了孔洞缺陷的产生。
关键词: 贝氏体型非调质钢FAS2225, 铸坯, 加热, 中心开裂, 热应力, 组织应力, 预热温度
Yan Yan, Hao Yanying , Liu Xianda. An Analysis and Process Improvement on Hole-Defect of Hot-Rolled Billet of Non-Quenched and Tempered Bainite Steel FAS2225[J]. Special Steel, 2018, 39(2): 41-43.
阎岩, 郝彦英, 刘献达. 贝氏体非调质钢FAS2225轧坯孔洞缺陷分析及工艺改进[J]. 特殊钢, 2018, 39(2): 41-43.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2018/V39/I2/41