ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2017, Vol. 38 ›› Issue (6): 60-62.

Previous Articles     Next Articles

Effect of Ti and Normalizing Process on Low Temperature Impact Toughness of Nb-V-Ti Microalloying Steel 16MnT for Motor Shaft

Wu Zhonghua, Chen Jinhu, Qiao Xiaomei , Chu Baoshuai   

  1. Technology Center, Shanxi Taigang Stainless Steel Co Ltd, Taiyuan 030003
  • Received:2017-06-08 Online:2017-12-01 Published:2022-07-15

Ti和正火工艺对Nb-V-Ti微合金电机轴用钢16MnT低温冲击韧性的影响

邬中华,陈金虎,乔晓梅,楚宝帅   

  1. 山西太钢不锈钢股份有限公司技术中心,太原030003
  • 作者简介:邬中华(1978-),男,硕士(2008年北京科技大学),工程师, 2001年武汉科技大学(本科)毕业,碳钢型线材新产品开发工作。

Abstract: The production process flowsheet of tested steel 16MnT (/%: 0.14~0.15C, 0.27〜0.30Si, 1.40Mn, 0.008~0.010P, 0.003~0.004S, 0.020~0.025Nb, 0.10V, 0.002〜0.08Ti, 0.025~0.027Al, 0.0043~0.0053N) is 60t EAF-LF-VD-5.8 t ingot casting-Ф190~250mm forging- normalizing at 920℃. Examination results show that the impact energy of forged-normalized 0.08%Ti steel 16MnT at -20°C is 6~16J, it is lower than the value of standard requirement-34J. The analysis results obtain that large amount TiN and along grain boundary precipitated phase Nb-Ti ( C, N) exist in 0.08%Ti steel and the fracture of steel at -20T is typical brittle fracture along grain boundary, and the structure of forged product section is non-homogeneous, at surface it is sorbite while at centre of section it is ferrite+pearlite. With decreasing the Ti content in steel to 0.002% and controlling the 1.5m distance between forgings during normalizing wind-fog cooling process, the impact energy of forged product of steel 16MnT at -20℃ increases to 132~288J.

摘要: 试验16MnT钢(/%:0.14~0.15C,0.27~0.30Si,1.40Mn,0.008~0.010P,0.003~0.004S,0.020~0.025Nb,0.10V,0.002~0.08Ti,0.025~0.027Al,0.0043~0.0053N)的生产工艺流程为60t EAF-LF-VD-5.8t铸锭-锻造Ф190~250mm棒材-920℃正火。检验结果表明,0.08%Ti 16MnT钢锻造正火后-20℃冲击功为6~16J,低于标准值34J。分析结果得出,0.08%Ti钢中存在大量TiN和延晶Nb-Ti(C,N)析出相,-20℃钢的断口为典型沿晶脆性断裂,且锻材断面的组织不均匀,表面为索氏体,心部为铁素体+珠光体。通过将钢中Ti含量降至0.002%,正火风雾冷却时锻材间距离为1.5m,使16MnT钢锻材的-20℃冲击功提高至132~288J。

关键词: Ti, 微合金电机轴用钢16MnT, 锻材, 正火工艺, 低温冲击性能