ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2017, Vol. 38 ›› Issue (5): 40-43.

Previous Articles     Next Articles

Effect of Casting Electromagnetic Stirring and Light Reduction on Metallurgical Quality of Gas Cylinder Steel 34CrMo4

Lu Bingjun1 , Qi Feng1  , Shen Wanlin2 , Liu Jun3   

  1. 1. Products Research Institute, Benxi Steel Plates Co Ltd, Benxi 117000;
    2. Jiaozuo Jinxin Hengtuo Advanced Materials Co Ltd, Jiaozuo 454450;
    3. Steel Plant, Benxi Steel Plates Co Ltd, Benxi 117000;
  • Received:2017-04-27 Online:2017-10-01 Published:2022-07-15

连铸电磁搅拌和轻压下对气瓶钢34CrMo4冶金质量的影响

卢秉军1,齐峰1,沈万林2,刘军3   

  1. 1. 本钢板材股份有限公司产品研究院,本溪 117000;
    2. 焦作金鑫恒拓新材料股份有限公司,焦作 454450;
    3. 本钢板材股份有限公司炼钢厂,本溪 117000;
  • 作者简介:卢秉军(1972-),男,教授级高级工程师,1993年辽宁工学院毕业,特殊钢产品研究与开发。

Abstract: The production flowsheet for gas cylinder steel 34CrMo4 is hot-metal pretreatment- 180 t BOF- LF- RH- 350 mm x 470 mm blooms casting. The pilot production is carried out on 4-strands casting respectively by using mold electromagnetic stirring ( M-EMS, 480 A, 2 Hz) ; M-EMS + solidification end electromagnetic stirring ( E-EMS, 320 A, 6 Hz) ; M-EMS + light reduction ( LR, 3 mm-4 mm-3 min) and M-EMS + E-EMS + LR process, it is obtained that the process with M-EMS (480 A, 2 Hz) + E-EMS (320 A, 6 Hz) + 3-4-3(mm) light reduction is available to improve the internal metallurgical quality of casting bloom. 9 heats commercial production results show that the tensile strength of gas cylinder steel 34CrMo4 steelmaking by the flowsheet is up to 1070 〜1159 MPa and oxygen content in steel is ≤0.0020% , and by using M-EMS + E-EMS + LR casting process the steel has high density and the rating of center porosity of bloom is ≤1.0.

Key words: Gas Cylinder Steel 34CrMo4, 180 t BOF-LF-RH-CC Flowsheet, Electromagnetic Stirring, Light Reduction, Centrer Porosity

摘要: 气瓶钢34CrMo4的生产工艺流程为铁水预处理-180 t BOF-LF-RH-350 mm×470 mm坯连铸。对4流连铸分别采用结晶器电磁搅拌(M-EMS,480 A,2 Hz);M-EMS+凝固末端电流搅拌(E-EMS,320 A,6 Hz);M-EMS+轻压下(LR,3 mm-4 mm-3 mm)以及M-EMS+E-EMS+LR进行工业试验,得出M-EMS(480 A,2 Hz)+E-EMS(320A,6 Hz)+3-4-3(mm)轻压下工艺,有效提升连铸坯内部冶金质量。9炉生产结果表明,该流程生产的气瓶钢34CrMo4的抗拉强度达1070~1159 MPa,钢中氧含量≤0.0020%,采用M-EMS+E-EMS+LR连铸工艺时,该钢具有高致密度,铸坯中心疏松级别≤1.0。

关键词: 气瓶钢34CrMo4, 180t BOF-LF-RH-CC流程, 电磁搅拌, 轻压下, 中心疏松