ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2016, Vol. 37 ›› Issue (6): 13-16.

Previous Articles     Next Articles

Effect of Spread Model for Steel Q345 on Predicted Calculated Precision of Medium and Heavy Plate Rolling Load

Xiao Zhiyu1, Li Lirong2, Liu Bing1,Liu Xiaoning1   

  1. 1 Wuhan Software and Engineering Profession College, Wuhan 430205 ;
    2 Wuhan College, Zhongnan University of Economics and Law, Wuhan 430079
  • Received:2016-06-27 Online:2016-12-01 Published:2022-07-25

Q345钢宽展模型对中厚板轧制压力预算精度的影响

肖志余1,李丽容2,刘 兵1,刘小宁1   

  1. 1武汉软件工程职业学院,武汉430205;
    2中南财经政法大学武汉学院,武汉430079
  • 作者简介:肖志余(1982-),女,硕士(2011年武汉科技大学),讲师,2005年安徽工业大学(本科)毕业,轧制过程计算机控制和 模具设计研究。

Abstract: With established calculated spread model for test medium and heavy plate rolling process, the predicted calculation on rolling load for steel Q345 (/% : ≤0.20C, ≤1.60Mn, ≤0.55Si) in each rough rolling pass by 10 passes rolling from 210 mm casting slab to 48 mm plate has been carried out and the effect of test spread model and Besse spread model on medium and heavy plate rolling load is analyzed. Results show that in medium and heavy plate initial 2 and 3 pass and last 9 and 10 pass the predicted precision of rolling load calculated by test spread model is higher, its relative error is 0. 26% ~0. 68% , in 4 ~ 8 passes the predicted precision of rolling load calculated by Besse spread model is higher, its relative error is 0. 33%~11. 79% , and for the two models all the relative error in first pass is 18. 00%.

摘要: 通过建立的实验中厚板轧制过程宽展计算模型,对Q345钢(/%:≤0.20C,≤1.60Mn,≤0.55Si)中厚板210 mm铸坯经10道次轧成48 mm板的各粗轧道次轧制压力进行预算,分析试验宽展模型和Besse宽展模型对中厚板轧制压力的影响。结果表明,在中厚板轧制开始23道次和终止910道次,实验宽展模型轧制压力预算精度较高,相对误差为0.26%~0.68%;轧制48道次,Besse宽展模型轧制压力预算精度较高,其相埘误差为0.33%~11.79%,两模型第1道次的相对误差均为18.00%。