Analysis on Thermodynamics of Behavior of Inclusions in Stainless Steel 316L during LF Refining and Process Optimization

Li Jidong1,2, Han Peide1 , Wang Feng2, Ren Yongxiu2 , Jia Yuanwei2   

  1. 1 College of Materials Science and Engineering, Taiyuan University of Science and Engineering, Taiyuan 030024 ;
    2 Technology Center, Shanxi Taigang Stainless Steel Co Ltd, Taiyuan 030003
  • Received:2016-07-21 Online:2017-02-01 Published:2022-07-28

316L不锈钢LF精炼过程夹杂行为热力学分析和工艺优化

李吉东1,2, 韩培德1,王 烽2, 任永秀2, 贾元伟2   

  1. 1太原理工大学材料科学与工程学院,太原030024;
    2山西太钢不锈钢股份有限公司技术中心,太原030003
  • 作者简介:李吉东(1982-),男,工程师,2007年东北大学(本科)毕业, 不锈钢精炼研究。

Abstract: The diagrams of forming MgO ·Al2O3, 2MgO·SiO2, 3Al2O3 , 2SiO2 and 2MgO·2Al2O3 ·5SiO2 phase predominance area during refining process of stainless steel 316L (/% : 0. 02C, 0. 51 Si, 1. 15Mn, 0. 030P, .001S, 16. 77Cr, 10. 12Ni, 2. 07Mo, 0. 040N, 0. 006Ti, 0. 004Al) in equilibrium condition after deoxidation are obtained by using thermodynamic calculation method, and the thermodynamic conditions for formation and transformation of various inclusions have been studied and analyzed. Results show that at 1 873 K as the solution Al content in liquid is less than 0. 001 % and the solution Mg content is less than 2 x 10-7% , it is available to form the better deformable 2MgO·2Al2O3·5SiO2 low-melting-point inclusions; as solution Al content in liquid is less than 1. 7 x 10-4 % , there is no spinel inclusions MgO·Al2O3 formed in liquid ; and the formation area of high-melting-point inclusions 2MgO ·SiO2 and 3Al2O3 , 2SiO2 is largest. Practice results show that the thermodynamic condition for modification treatment on high-melting-point inclusions 2MgO · SiO2 and 3Al2O3·2SiO2 by adding Ca is sufficient, as solution oxygen content in 180 t LF liquid of stainless steel 316L is 0. 002 0% , the refining end[O] is 0. 001 5% by feeding silicon-calcium wire 2 m/t, and the rating of C-type inclusions in 2mm cold rolled sheet is 0. 5 ~ 1. 0, the main composition of inclusions is CaO·Al2O3·SiO2.

摘要: 采用热力学计算方法得出316L不锈钢(/%:0.02C,0.51Si,1.15Mn,0.030P,0.001S,16.77Cr,10.12Ni,2.07Mo,0.040N,0.006Ti,0.004Al)精炼过程中脱氧平衡后形成MgO·Al2O3、2MgO·SiO2、3Al2O3·2SiO2、2MgO·2Al2O3·5SiO2优势区图,研究和分析了各类夹杂物生成与转变的热力学条件。结果表明,在1 873 K时,当钢液中的溶解Al含量低于0.001%和溶解Mg含量低于2×10-7%时才能形成低熔点变形能力较好的2MgO·2Al2O3·5SiO2类夹杂物;当钢液中溶解Al含量在1.7×10-4%以下,钢液中不形成MgO·Al2O3尖晶石夹杂;2MgO·SiO2与3Al2O3·2SiO2类高熔点夹杂物形成区域最大。实践表明,加Ca对高熔点夹杂物2MgO·SiO2与3Al2O3·2SiO2变性处理的热力学条件充足,当316L不锈钢180 t LF钢液溶解氧为0.002 0%,进行喂硅钙线2 m/t,精炼终点[O]为0.001 5%,2 mm冷轧板夹杂物为C类0.51.0级,主要成分为CaO·Al2O3·SiO2。