Abstract: Process flowsheet of test heavy gear steel 18CrNiMo7-6 (/% : 0.165C , 0.59Mn, 0.24Si, 0.006S, 0.008P, 1.56Ni, 1.71Cr, 0.28Mo, 0.034Al, 0.0129N) is 60 t UHP EAF-LF-VD-12.5 t ingot casting process. The effect of ingot heating process (1200-1220 °C , 7-8 〜13-15 h) , forged product complete annealing (900 °C 12 h, with ≤ 80 °C/h slow cooling to 650 °C 50 h, air cooling) , isothermal annealing (900 °C 12 h, air cooling to 650 °C 50 h, air cooling) and normalizing (900 °C 12 h, air cooling) process on banded structure of Φ540 mm forged bar has been tested and studied. Results show that as ingot heating at 1200-1220 °C for 7-8 h, the rating of banded-structure of forged bar by complete annealing, isothermal annealing or normalizing process is respectively 4.0, 3.5 and 3.0, while as ingot heating at 1200-1220 °C for 13-15 h, then normalized, the rating of banded-structure of forged bar is 2.5 , it is an optimum process.
Key words: Gear Steel 18CrNiMo7-6, Φ540 mm Forged Bar, Ingot High Temperature Diffusion Process, Normalizing, Annealing, Banded-Structure
摘要: 试验18CrNiMo7-6重型齿轮钢(/%:0.165C,0.59Mn,0.24Si,0.006S,0.008P,1.56Ni,1.71Cr,0.28Mo,0.034M,0.0129N)的生产流程为60 t UHP EAF-LF-VD-12.5 t铸锭工艺。试验研究了钢锭加热工艺(1200~1220℃,7-8 h~13-15 h),锻材完全退火(900℃ 12 h,≤80℃/h至650℃50 h,空冷)、等温退火(900℃ 12 h,空冷至650℃50 h,空冷)和正火(900℃ 12 h,空冷)工艺对Φ540 mm锻材带状组织的影响。结果表明,钢锭1200~1220℃ 7-8 h加热,锻材经完全退火、等温退火或正火处理后其带状级别分别为4.0,3.5和3.0,钢锭经1200~1220℃ 13-15 h加热,锻材经正火处理后其带状级别为2.5,为最佳工艺。
关键词: 18CrNiMo7-6齿轮钢, Φ540 mm锻材, 铸锭高温扩散, 正火, 退火, 带状组织
Liu Jinxin , Zhao Min , Feng Guiping , Zhao Zhigang , Cheng Lijie , Yu Zhongyang. Effect of Ingot Heating and Forged Products Heat Treatment Process on Banded-Structure of Φ540 mm Bar of Steel 18CrNiMo7-6[J]. Special Steel, 2015, 36(2): 62-63.
刘金鑫, 赵敏, 冯桂萍, 赵智刚, 程丽杰, 于忠洋. 铸锭加热和锻后热处理工艺对18CrNiMo7-6钢Φ540 mm棒材带状的影响[J]. 特殊钢, 2015, 36(2): 62-63.