Experimental Study on Hydraulic Model of Coherent Jet Flow Field in 180 t Converter

Bao Liming1, Liu Kun2 , Lü Guocheng1   

  1. 1 Metallurgical Institute, Jilin Technology Profession College of Electronic Information, Jilin 132021;
    2 School of Material and Metallurgy, Liaoning University of Science and Technology, Anshan 114044
  • Received:2013-12-27 Online:2014-06-01 Published:2022-08-27

180 t转炉聚合射流流场的水力学模型的实验研究

包丽明1,刘坤2,吕国成1   

  1. 1吉林电子信息职业技术学院冶金学院,吉林132021,
    2辽宁科技大学材料与冶金学院,鞍山114044
  • 作者简介:包丽明(1983-),女,硕士(辽宁科技大学),讲师,2006年辽宁科技大学(本科)毕业,冶金工艺研究。

Abstract: Simulation test on interaction between jet flow and bath in 180 t top and bottom combined blowing converter has been carried out by a water model with geometric similarity ratio 1:10 to study the effect of gas flow rate (38 ~42 m3/h) on mixing time with optimum lance position (150 mm) and the effect of coherent jet flow lance position (40 ~ 150 mm) on mixing time at optimum top lance flow rate (39 m3/h). Results show that the stirring effect in bath by coherent jet flow oxygen lance is the same as that by top and bottom combined blowing and if the coherent jet flow oxygen lance shall be applied in converter, the bottom system of top and bottom combined blowing converter could be canceled to simplify converter structure and increase converter lining life.

摘要: 采用几何相似比1∶10水模型对180 t顶底复吹转炉内射流与熔池相互作用进行模拟试验,研究了在最佳枪位(150 mm)时氧气流量(38~42 m3/h)对均混时间的影响以及最佳顶枪流量(39 m3/h)下聚合射流氧枪枪位(40~150 mm)对均混时间的影响。结果表明,聚合射流氧枪对熔池的搅拌效果完全能达到顶底复吹的搅拌效果,如能在转炉冶炼工艺中应用,可取消底吹系统,简化转炉设备,提高转炉炉龄。