Effect of Nitrogen Content on Behavior of Elevated Temperature Deformation of Austenite Stainless Steel 1Cr17Mn6Ni5N

Yang Jichun1, Gao Fubin1,2 , Li Yanfeng2   

  1. 1 School of Material and Metallurgy, Inner Mongolia University of Science and Technology, Baotou 014010 
    2 No.2 Steelmaking Plant, Chengde Steel Co, Hebei Iron and Steel Group, Chengde 067102
  • Received:2013-12-21 Online:2014-06-01 Published:2022-09-01

氮含量对1Cr17Mn6Ni5N奥氏体不锈钢高温变形行为的影响

杨吉春1,高福彬1,2,李艳峰2   

  1. 1内蒙古科技大学材料与冶金学院,包头014010;
    2河北钢铁集团承钢公司炼钢二厂,承德067102
  • 作者简介:杨吉春(1963-),男,博士,教授,1984年包头钢铁学院(本科)毕业,稀土在钢中的应用研究。
  • 基金资助:
    国家自然科学基金资助项目(51364031)

Abstract: The test steel 1Cr17Mn6Ni5N (/% : 0. 09 ~ 0.11C, 0.19 ~ 0.29Si, 7.33~7.42Mn, 0.011 -0.015P, 0. 004 ~ 0. 007S, 16. 87 ~ 17. 24Cr, 5. 06 ~5.19Ni, 0. 21 ~0. 40N) is melted by a 10 kg vacuum induction furnace with adding chromium nitride to N-alloying in nitrogen atmosphere. The compression 60% experiment of test steel in vacuum with strain rate 10-2 s-1 and 1 s-1 at 1 150 ~ 1 000 ℃ has been carried out by using Gleebl-1500D thermo-mechanical simulation machine. Test results show that at high temperature with lower strain rate the dynamic recrystallization of steel is main softening mechanism and with higher strain rate the dynamic recovery of steel is the main softening mechanism as compared with 0. 21 % N and 0.29% N test steels the 0. 40% N test steel has higher peak stress, and based on the calculation of Zener-Hollomon parameter, the recrystallization activation energy of 0. 40% N test steel is highest, uneasily to happen dynamic crystallization at elevated temperature.

摘要: 试验用1Cr17Mn6Ni5N钢(/%:0.09~0.11C,0.19~0.29Si,7.33~7.42Mn,0.011~0.015P,0.004~0.007S,16.87~17.24Cr,,5.06~5.19Ni,0.21~0.40N)由10kg真空感应炉熔炼,通过氮气气氛加氮化铬进行N合金化。通过Gleeble-1500D热模拟试验机将实验钢在真空下1150~1 000℃,以应变速率10-2s-1和1 s-1进行压缩60%试验。结果表明,在高温下,以低应变速率压缩时钢的动态再结晶是主要的软化机制;以高应变速率压缩时钢的动态回复是主要的软化机制;与0.21%N和0.29%N试验钢相比,含0.40%N的试验钢具有较高的峰值应力,根据Zener-Hollomon参数的计算得出0.40%N的试验钢再结晶激活能最高,在高温下不易发生动态再结晶。