Effect of Austempering on Mechanical Properties of 700 MPa Cold Rolled TRIP Steel 0.15C-1.5Mn-l. 4Si-0. 03Nb-0.03Ti-0.005N

Yao Chunfa 、 Li Guangying   

  1. Central Iron and Steel Research Institute, Beijing 100081
  • Received:2013-08-17 Online:2014-02-01 Published:2022-09-06

等温淬火对 700 MPa 冷轧 TRIP 钢 0.15C-1. 5Mn-l. 4Si-0. 03Nb-0. 03Ti-0. 005N力学性能的影响

姚春发、李光瀛   

  1. 钢铁研究总院,北京100081
  • 作者简介:姚春发(1964-),男,高级工程师,北京化工大学(本科)毕业,产品开发研究。

Abstract: Test steel is melted by a 50 kg vacuum induction furnace, forged to 60 mm slab, homogenized at 1 250 ℃ then hot-rolled to 4 mm plate and cold rolled to 1 mm sheet. The effect of austempering temperature (350 ~ 450 °C) and holding time (1 ~ 10 min) on structure and mechanical properties of 820℃ 3 min quenched test TRIP steel cold-rolled sheet has been studied. Results show that the effect of process of austempering on mechanical properties of test steel is obvious; the optimum austempering process is 820℃ 3 min +400℃ 5 min, water cooling, the tensile strength and total elongation are respectively 766 MPa and 37%, i. e. the strength-plasticity product is 28. 34 GPa , % ; a lot of Nb (CN) particles precipitation with 10 nanometer size is main factor to increase the strength of test steel.

摘要: 试验钢由50 kg真空感应炉冶炼,锻造成60 mm板坯经1 250℃均匀化处理后热轧至4 mm板,再冷轧至1 mm板。研究了试验TRIP(转变诱发塑性)钢冷轧板820℃3 min淬火时等温淬火温度(350~450℃)和保温时间(1~10 min)对钢的组织性能的影响。结果表明,奥氏体等温淬火工艺对试验钢的力学性能有显著影响;最佳的等温淬火工艺为820℃3 min+400℃5min水冷,该钢的抗拉强度与总伸长率分别为766 MPa与37%,即强塑积达28.34 GPa·%;10 nm级Nb(CN)粒子的大量析出是造成该试验钢强度显著提高的主要原因。