Numerical Simulation of a New Type Submerged Entry Nozzle for 200 mm x 200 mm Billet Continuous Casting
Chen Yuanqing1,2 , Shang Zhenghong1 , Tao Naibiao1 , Wang Jin1 , Qiu Shengtao2
1. Zhangjiagang Lianfeng Iron & Steel Research Institute Co Ltd, Zhangjiagang 215628;
2. National Engineering and Research Center for Continuous Casting Technology, Central Iron and Steel Research Institute, Beijing 100081;
Chen Yuanqing , Shang Zhenghong , Tao Naibiao , Wang Jin , Qiu Shengtao. Numerical Simulation of a New Type Submerged Entry Nozzle for 200 mm x 200 mm Billet Continuous Casting[J]. Special Steel, 2014, 35(2): 13-15.
[1] 文光华,唐萍,苏振江,等.k 方坯连铸结船器伸人式水II结 构类型研究[J].钢铁机钛, 2002,23(3) :2l-24.
[2] 顾武安,唐 萍,文光华,等.大 方坯连铸四孔浸入式水II的应 用研究[J].钢铁,2008,43(4): 101-104.
[3] 幸伟,沈巧珍.方坯连铸结品器枝人式水II結构类型的研究 [J].钢铁研究,2004(5):24-27.
[4] 吴国文,李明晓.4孔浸入式水11结M器钢水流场的仿真分析及其在连铸牛:产中的应川[J].特殊钢,2009,30(3) :4647.
[5] 吴機光,陈远清,仇圣桃,等.大圆坯连铸用新型旋流水口的数值模拟[J].钢铁钒钛,2009,30(4):49-54.
[6] Kholmatov S,Takagi S, Jonsson L,et al. Development of Flow Field and Temperature Distribution during Changing Divergent Angle of the Nozzle When Using Swirl Flow in a Square Continuous Casting Billet Mould[J].ISIJ International,2007,47(1):80-87.