ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2013, Vol. 34 ›› Issue (4): 19-21.

Previous Articles     Next Articles

Thermodynamic Process of Reaction System of MgO-C-S (FeS)

Liu Kun, Gao Xin, Xing Fei, Zhao Qi , Liu Yizhou   

  1. School of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051
  • Received:2013-01-14 Online:2013-08-01 Published:2022-09-11

MgO-C-S ( FeS)反应的热力学过程

刘坤,高鑫,邢飞,赵奇,刘宜州   

  1. 辽宁科技大学材料与冶金学院,鞍山H4051
  • 作者简介:刘 坤( 1965-).女.博士,教授,1987年鞍山钢铁学院毕业.冶金传输工程.冶金资源综合利用
  • 基金资助:
    辽宁省镁资源办资助项目(2011801);
    辽宁省“大学 生创新创业训练计划”项目(201210146004);
    高等学 校博士点专项科研基金资助项目(20102120120001)

Abstract: With using Setsys Evolution synchronous thermal analysis system the thermodynamic process of reaction of MgO-C-S (FeS) on 3 kinds of scheme- (1 ) magnesium oxide + carbon powder + sulphur , ( 2 ) magnesium oxide + carbon powder + ferrous sulfide and (3 ) magnesium oxide + carbon powder + ferrous sulfide + aluminum powder + hematite (Fe2O3) with heating rate 10 ~25 °C/min nitrogen atmosphere at 1 350 ℃ has been tested and researched to get differential thermal-thermo gravimetric curves. Results show that the reaction temperature of MgO-C-FeS system is lower than that of MgO-C-S system, and with adding thermite in MgO-C-FeS system the reaction of system shall be moved up.

摘要: 采用Setsys Evolution同步热分析系统对(1)氧化镁+碳粉+单质硫,(2)氧化镁+碳粉+硫化亚铁,(3)氧化镁+碳粉+硫化亚铁+铝粉+赤铁矿(Fe2O3) 3种试验方案以10~25℃/min的升温速度在1 350℃氮气中试验研究了MgO-C-S(FeS)反应的热力学过程,得出差热-热重曲线。结果表明,MgO-C-FeS体系的反应温度要低于MgO-C-S体系的反应温度,在MgO-C-FeS体系中加入发热剂,会使体系的反应提前。