A Study on 80 t Converter-Ladle Furnace Refining Slag for High Quality GCrl5 Bearing Steel Steelmaking

Liu Fayou, Xu Zhigang, Shang Ming   

  1. Shandong Shouguang Juneng Special Steel Co Ltd, Shouguang 262711
  • Received:2012-07-29 Online:2013-02-01 Published:2022-09-13

高品质GCrl5轴承钢80 t转炉-钢包炉精炼渣的研究

刘发友, 徐志刚, 尚明   

  1. 山东寿光巨能特钢有限公司,寿光262711
  • 作者简介:刘发友(1970-),男,硕士,高级工程师,辽宁科技大学冶金工程专业,钢铁冶金研究。

Abstract: Steelmaking flow sheet for GCrl5 bearing steel is 80 t top and bottom combined blowing converter-LF refi- ning-VD-180 mm x 220 mm CC process. The effect of CaO-SiO2 -Al2 03 -CaF2 -MgO refining slag series with basicity 3 ~ 8 on metallurgy quality of high quality GCrl5 bearing steel (/% : 0. 95 ~ 1. 05C, 0. 15 ~0. 35Si, 0. 25 ~0. 45Mn, 1. 40 ~ 1,65Cr, W0. 025P, W0. 025S, WO.001 2[ 0]) is studied. Commercial production results show that with using 5. 8 basicity refining slag (/% : 50 ~55CaO, 6 ~ 12SiO2, 15A12O3, 10CaF2, W0. 5FeO, W8MgO) , it is available to decrease the oxygen content and inclusions in steel, the oxygen content in GCrl5 bearing steel is (5 ~9) x 10-6 , average oxygen content is 5. 6 x 10-6 , the sulphur content in steel is 0. 005% ~ 0. 009% , and the rating of inclusion in steel is 0 ~ 0. 5.

摘要: GCr15轴承钢的冶炼流程为80 t顶底复吹转炉-LF精炼-VD-180 mm×220 mm连铸工艺。研究了碱度3~8的CaO-SiO2-Al2O3-CaF2-MgO精炼渣系对高品质GCr15轴承钢(/%:0.95~1.05C、0.15~0.35Si、0.25~0.45Mn、1.40~1.65Cr、≤0.025P、≤0.025S、≤0.001 2[O])冶金质量的影响。生产结果表明,采用碱度5.8的精炼渣(/%:50~55CaO、6~12SiO2、15Al2O3、10CaF2、≤0.5FeO、≤8MgO)可有效地降低钢中氧含量和夹杂物,GCr15轴承钢的氧含量为(5~9)×10-6,平均氧含量为5.6×10-6,硫含量达0.005%~0.009%,夹杂物0~0.5级。